Final Magnetic Moment2.370 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.903 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.230 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTi3O5 + TiVO3 + LiTi2O4 + V |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 -1> | 342.8 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 174.4 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 173.4 |
AlN (mp-661) | <1 0 1> | <0 1 -1> | 120.8 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 271.8 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 138.7 |
BaF2 (mp-1029) | <1 0 0> | <1 -1 1> | 319.6 |
BaF2 (mp-1029) | <1 1 1> | <0 1 -1> | 211.4 |
GaN (mp-804) | <0 0 1> | <1 1 -1> | 244.9 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 233.7 |
GaN (mp-804) | <1 1 1> | <1 -1 -1> | 148.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 273.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 148.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 139.5 |
KCl (mp-23193) | <1 0 0> | <1 -1 1> | 319.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 230.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 138.7 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 173.4 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 288.9 |
LiF (mp-1138) | <1 1 0> | <1 1 -1> | 49.0 |
Te2W (mp-22693) | <0 1 1> | <1 1 -1> | 293.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 151.8 |
YVO4 (mp-19133) | <1 0 1> | <1 1 0> | 287.8 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 173.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 -1> | 211.4 |
Te2Mo (mp-602) | <1 0 1> | <0 1 -1> | 271.8 |
Te2Mo (mp-602) | <1 1 0> | <1 -1 1> | 284.0 |
Ag (mp-124) | <1 0 0> | <1 -1 1> | 35.5 |
Ag (mp-124) | <1 1 1> | <0 1 -1> | 30.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 -1> | 120.8 |
GaSe (mp-1943) | <0 0 1> | <0 1 -1> | 90.6 |
GaSe (mp-1943) | <1 0 0> | <0 1 -1> | 271.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 277.5 |
CeO2 (mp-20194) | <1 1 1> | <0 1 -1> | 211.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 99.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 138.7 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 173.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 151.8 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 173.4 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 90.6 |
KCl (mp-23193) | <1 1 1> | <0 1 -1> | 211.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 99.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 208.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 347.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 312.2 |
InAs (mp-20305) | <1 0 0> | <1 -1 1> | 319.6 |
InAs (mp-20305) | <1 1 1> | <0 1 -1> | 211.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 99.2 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 173.4 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 1> | 142.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgTi2O4 (mvc-16746) | 0.2171 | 0.102 | 3 |
Ti2ZnO4 (mvc-16752) | 0.2160 | 0.303 | 3 |
MgV2O4 (mvc-16820) | 0.2158 | 0.242 | 3 |
Al(NiS2)2 (mvc-16791) | 0.2169 | 0.198 | 3 |
Li2CoCl4 (mp-22980) | 0.2131 | 0.018 | 3 |
LiTiFeO4 (mp-762701) | 0.2740 | 0.097 | 4 |
Li4Fe3Co5O16 (mp-763071) | 0.3158 | 0.094 | 4 |
LiFeCoO4 (mp-853174) | 0.3171 | 0.382 | 4 |
Li2Cr3CoO8 (mp-763336) | 0.3287 | 0.081 | 4 |
Li2MnFe3O8 (mp-768068) | 0.3210 | 0.090 | 4 |
Fe3O4 (mp-612405) | 0.3202 | 0.876 | 2 |
Ti3O4 (mp-755875) | 0.2635 | 0.058 | 2 |
Ni3Cl4 (mp-1096772) | 0.2421 | 0.076 | 2 |
Ni3Cl4 (mp-1096769) | 0.1867 | 0.045 | 2 |
Ni3Cl4 (mp-1096770) | 0.2592 | 0.076 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv V_pv O |
Final Energy/Atom-8.2497 eV |
Corrected Energy-122.6914 eV
Uncorrected energy = -115.4954 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-1.700 eV/atom x 1.0 atoms) = -1.7000 eV
Corrected energy = -122.6914 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)