Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.265 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiPO4 |
Band Gap3.656 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 80.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 60.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 261.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 100.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 241.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 60.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 261.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 60.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 261.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 261.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 161.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 261.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 100.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 241.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 60.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 80.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 60.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 342.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 261.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 261.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 100.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 141.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 261.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 302.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 181.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 80.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 141.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 100.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 261.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 261.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 241.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 322.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 261.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 261.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 241.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 80.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 322.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 60.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 322.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 322.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 60.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 322.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 322.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 322.3 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 80.6 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 362.6 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 197.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 141.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 100.7 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 261.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Cr2O5 (mp-1099683) | 0.6637 | 0.187 | 3 |
Sr2In2O5 (mp-22512) | 0.6845 | 0.029 | 3 |
Ca2Fe2O5 (mp-1076319) | 0.7094 | 0.047 | 3 |
Ca2Ga2O5 (mp-16433) | 0.6660 | 0.034 | 3 |
Ca2Al2O5 (mp-10444) | 0.7175 | 0.023 | 3 |
LiCoPO4 (mp-765409) | 0.0732 | 0.085 | 4 |
LiMnPO4 (mp-766155) | 0.4014 | 0.075 | 4 |
LiVPO4 (mp-850484) | 0.2419 | 0.053 | 4 |
Ca2MnAlO5 (mp-18907) | 0.6220 | 0.011 | 4 |
Ca2MnGaO5 (mp-25018) | 0.6096 | 0.003 | 4 |
K2Mn3V2(HO5)2 (mp-762295) | 0.7215 | 0.000 | 5 |
MnVHPbO5 (mp-762162) | 0.6630 | 0.000 | 5 |
NaZnMoHO5 (mp-540607) | 0.7366 | 0.007 | 5 |
VZnHPbO5 (mp-745150) | 0.6567 | 0.000 | 5 |
K3V2P2O8F3 (mp-1097033) | 0.6499 | 0.077 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv P O |
Final Energy/Atom-6.2533 eV |
Corrected Energy-97.4918 eV
-97.4918 eV = -87.5455 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 4.3280 eV (MP Advanced Correction)
|