material

VOF

ID:

mp-754072


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-2.833 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.012 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.41 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
VOF
Band Gap
1.580 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiC (mp-11714) <1 0 1> <0 1 0> 0.013 129.7
CdS (mp-672) <1 0 1> <0 1 0> 0.029 129.7
Bi2Se3 (mp-541837) <0 0 1> <0 1 0> 0.039 181.6
MgF2 (mp-1249) <1 0 1> <1 1 -1> 0.047 291.1
InP (mp-20351) <1 0 0> <1 1 1> 0.055 142.9
Te2Mo (mp-602) <1 0 1> <1 1 1> 0.055 333.5
TeO2 (mp-2125) <0 1 0> <0 1 0> 0.056 207.5
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.056 229.6
LiGaO2 (mp-5854) <1 1 0> <1 0 -1> 0.066 97.5
GdScO3 (mp-5690) <1 0 0> <1 0 1> 0.067 279.7
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.087 127.6
PbS (mp-21276) <1 0 0> <1 1 1> 0.088 142.9
CaCO3 (mp-3953) <1 0 1> <0 0 1> 0.089 178.6
WSe2 (mp-1821) <1 1 1> <0 1 0> 0.093 259.4
LiF (mp-1138) <1 1 1> <0 0 1> 0.098 204.1
SiO2 (mp-6930) <1 1 0> <1 0 0> 0.101 285.9
BN (mp-984) <1 0 0> <0 0 1> 0.102 76.5
AlN (mp-661) <0 0 1> <1 0 -1> 0.105 195.0
Ge (mp-32) <1 1 1> <0 1 1> 0.111 291.1
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.113 127.6
MgF2 (mp-1249) <1 0 0> <1 1 1> 0.114 190.6
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.118 127.6
CdS (mp-672) <0 0 1> <0 1 0> 0.122 181.6
YVO4 (mp-19133) <0 0 1> <1 1 -1> 0.125 207.9
Te2Mo (mp-602) <0 0 1> <1 0 1> 0.127 199.8
Mg (mp-153) <0 0 1> <1 1 0> 0.127 183.6
YVO4 (mp-19133) <1 0 1> <1 1 -1> 0.127 207.9
C (mp-66) <1 0 0> <0 0 1> 0.137 25.5
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.141 119.9
TbScO3 (mp-31119) <1 0 0> <1 0 1> 0.141 279.7
Ni (mp-23) <1 1 1> <0 0 1> 0.142 127.6
CdWO4 (mp-19387) <1 1 0> <0 1 0> 0.142 207.5
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.145 127.6
BaTiO3 (mp-5986) <1 0 1> <0 1 0> 0.148 207.5
Ni (mp-23) <1 1 0> <1 0 0> 0.155 52.0
ZnO (mp-2133) <1 1 1> <0 0 1> 0.156 127.6
MoS2 (mp-1434) <0 0 1> <1 1 0> 0.159 183.6
WS2 (mp-224) <0 0 1> <1 1 0> 0.160 183.6
SrTiO3 (mp-4651) <1 1 1> <1 0 1> 0.160 279.7
C (mp-48) <0 0 1> <0 0 1> 0.164 127.6
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.165 229.6
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.166 204.1
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.168 204.1
MgO (mp-1265) <1 0 0> <1 1 1> 0.168 142.9
TiO2 (mp-2657) <1 1 0> <1 0 -1> 0.175 97.5
MoSe2 (mp-1634) <1 1 1> <0 1 1> 0.179 181.9
GaAs (mp-2534) <1 1 1> <0 1 1> 0.184 291.1
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.186 127.6
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.209 229.6
DyScO3 (mp-31120) <1 0 0> <1 0 1> 0.219 279.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BiOF (mp-753478) 0.2942 0.019 3
TiOF (mp-752496) 0.2335 0.072 3
TaNO (mp-4165) 0.3340 0.000 3
DySCl (mp-561307) 0.2945 0.000 3
ScOF (mp-4661) 0.2590 0.000 3
ZrO2 (mp-2858) 0.3421 0.000 2
HfO2 (mp-775757) 0.3028 0.010 2
ZrO2 (mp-776404) 0.2835 0.009 2
NdO2 (mp-755820) 0.3559 0.178 2
CeSe2 (mp-1080303) 0.3332 0.024 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
V: 3.25 eV
Pseudopotentials
VASP PAW: V_pv O F
Final Energy/Atom
-7.1981 eV
Corrected Energy
-97.7737 eV
Uncorrected energy = -86.3777 eV Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV Composition-based energy adjustment (-0.462 eV/atom x 4.0 atoms) = -1.8480 eV Composition-based energy adjustment (-1.700 eV/atom x 4.0 atoms) = -6.8000 eV Corrected energy = -97.7737 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)