Final Magnetic Moment10.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.108 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Mn3GaO8 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 213.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 275.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 213.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 213.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 122.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 213.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 275.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 336.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 171.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 91.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 275.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 336.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 213.9 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 272.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 244.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 366.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 366.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 122.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 152.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 30.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 152.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 122.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 30.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 213.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 213.9 |
Te2Mo (mp-602) | <1 0 1> | <1 0 1> | 272.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 152.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 122.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 213.9 |
BN (mp-984) | <1 1 1> | <1 0 1> | 272.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 91.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 213.9 |
BN (mp-984) | <1 1 0> | <1 0 1> | 272.8 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 257.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 366.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 91.7 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 148.4 |
Al (mp-134) | <1 1 1> | <0 0 1> | 366.6 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 272.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 244.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 275.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 336.1 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 91.7 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 90.9 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 30.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 272.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 152.8 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 122.2 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 181.9 |
C (mp-66) | <1 0 0> | <0 0 1> | 152.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YCr2O4 (mvc-13339) | 0.0641 | 0.192 | 3 |
Mn6Cr9O20 (mp-761448) | 0.0725 | 0.036 | 3 |
Y(FeO2)2 (mvc-11640) | 0.0666 | 0.567 | 3 |
YTi2O4 (mvc-15302) | 0.0696 | 0.248 | 3 |
YTi2O4 (mvc-13097) | 0.0601 | 0.248 | 3 |
Li2Mn3CrO8 (mp-770321) | 0.0383 | 0.022 | 4 |
Li2Mn3FeO8 (mp-773283) | 0.0301 | 0.025 | 4 |
Li2TiCo3O8 (mp-775109) | 0.0634 | 0.206 | 4 |
Li2CoNi3O8 (mp-761777) | 0.0628 | 0.016 | 4 |
Li2Mn3VO8 (mp-772730) | 0.0472 | 0.072 | 4 |
Co3O4 (mp-559191) | 0.1404 | 0.046 | 2 |
In3S4 (mp-556597) | 0.1703 | 0.042 | 2 |
Co3O4 (mp-18748) | 0.0931 | 0.046 | 2 |
Sn3N4 (mp-16031) | 0.1905 | 0.000 | 2 |
Ge3N4 (mp-476) | 0.2244 | 0.109 | 2 |
Li4Cr2Fe3Co3O16 (mp-775698) | 0.3714 | 0.897 | 5 |
Li4Mn2Fe3Co3O16 (mp-761441) | 0.3815 | 0.078 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.3413 | 0.014 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.3486 | 0.069 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.3786 | 0.035 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Ga_d O |
Final Energy/Atom-6.6259 eV |
Corrected Energy-103.4230 eV
-103.4230 eV = -92.7621 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 5.0426 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)