Final Magnetic Moment4.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.314 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa2MnPCO7 |
Band Gap1.759 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 279.9 |
AlN (mp-661) | <1 1 0> | <1 1 -1> | 240.3 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 247.6 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 0> | 276.2 |
GaN (mp-804) | <0 0 1> | <1 0 -1> | 169.2 |
GaN (mp-804) | <1 1 0> | <1 -1 -1> | 116.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 256.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 247.6 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 256.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 209.9 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 1 0> | 247.6 |
Al (mp-134) | <1 1 0> | <1 0 1> | 256.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 247.6 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 165.8 |
MgO (mp-1265) | <1 1 0> | <1 -1 -1> | 232.4 |
Mg (mp-153) | <0 0 1> | <0 1 -1> | 167.0 |
LaF3 (mp-905) | <1 0 0> | <1 -1 0> | 276.2 |
LaF3 (mp-905) | <1 1 1> | <0 0 1> | 209.9 |
BaTiO3 (mp-5986) | <1 1 1> | <1 -1 -1> | 116.2 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 0> | 165.1 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 165.8 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 279.9 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 209.9 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 209.9 |
Au (mp-81) | <1 0 0> | <0 1 0> | 247.6 |
Au (mp-81) | <1 1 0> | <0 1 0> | 247.6 |
Au (mp-81) | <1 1 1> | <0 0 1> | 209.9 |
WS2 (mp-224) | <0 0 1> | <0 1 -1> | 167.0 |
C (mp-48) | <1 0 1> | <0 0 1> | 139.9 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 247.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 209.9 |
ZrO2 (mp-2858) | <0 1 0> | <1 -1 0> | 276.2 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 70.0 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 1> | 182.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 279.9 |
BN (mp-984) | <1 1 1> | <1 -1 0> | 276.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 -1> | 167.0 |
YAlO3 (mp-3792) | <0 0 1> | <1 -1 0> | 276.2 |
YAlO3 (mp-3792) | <0 1 1> | <1 -1 0> | 92.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 -1 0> | 276.2 |
LiTaO3 (mp-3666) | <1 0 0> | <1 -1 0> | 276.2 |
Mg (mp-153) | <1 1 0> | <1 -1 -1> | 116.2 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 247.6 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 247.6 |
PbS (mp-21276) | <1 1 1> | <0 1 0> | 247.6 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 247.6 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 247.6 |
TiO2 (mp-390) | <1 0 1> | <1 -1 -1> | 116.2 |
TiO2 (mp-390) | <1 1 1> | <0 0 1> | 209.9 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 247.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbCu2(MoO4)3 (mp-565220) | 0.7137 | 0.038 | 4 |
Na2NiPCO7 (mp-768089) | 0.2580 | 0.036 | 5 |
Na2NiPCO7 (mp-775744) | 0.2366 | 0.024 | 5 |
Na2MnPCO7 (mp-868618) | 0.0649 | 0.013 | 5 |
Na2MnPCO7 (mp-775643) | 0.2636 | 0.011 | 5 |
Na2MnPCO7 (mp-769485) | 0.0349 | 0.012 | 5 |
Na5LiNi2P2(CO7)2 (mp-770324) | 0.5690 | 0.009 | 6 |
Na2LiFePCO7 (mp-773940) | 0.5370 | 0.024 | 6 |
Na2LiFePCO7 (mp-773705) | 0.5505 | 0.025 | 6 |
NaLi2FePCO7 (mp-773689) | 0.6053 | 0.039 | 6 |
Na3Li3Fe2P2(CO7)2 (mp-773524) | 0.5775 | 0.030 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Mn_pv P C O |
Final Energy/Atom-6.8540 eV |
Corrected Energy-355.3801 eV
-355.3801 eV = -328.9926 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)