Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.267 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.876 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 258.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 73.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 129.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 184.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 206.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 323.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 110.9 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 253.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 147.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 129.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 258.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 193.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 -1> | 264.3 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 231.9 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 253.6 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 317.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 110.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 147.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 258.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 110.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 317.0 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 184.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 184.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 221.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 278.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 323.1 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 264.3 |
InAs (mp-20305) | <1 1 1> | <1 1 -1> | 264.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 193.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 332.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 231.9 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 143.0 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 285.9 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 147.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 332.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 165.3 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 231.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 258.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 214.4 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 110.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 214.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 258.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 206.1 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 317.0 |
Te2Mo (mp-602) | <1 1 0> | <0 1 1> | 190.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 258.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 193.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 258.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 258.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 323.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hg2SeO5 (mp-30123) | 0.6232 | 0.000 | 3 |
Li3Fe(BO2)5 (mp-761304) | 0.5804 | 0.048 | 4 |
Li3CrB4O9 (mp-761306) | 0.5870 | 0.089 | 4 |
CaGaBO4 (mp-557855) | 0.5294 | 0.000 | 4 |
Li3Mn(BO2)5 (mp-771291) | 0.5898 | 0.045 | 4 |
Li3MnB4O9 (mp-771178) | 0.5870 | 0.069 | 4 |
Na2AsPCO7 (mp-767546) | 0.3465 | 0.009 | 5 |
Li2SiSnCO7 (mp-770647) | 0.3317 | 0.084 | 5 |
K2SbPCO7 (mp-756981) | 0.3578 | 0.000 | 5 |
Li2AsPCO7 (mp-768153) | 0.3628 | 0.063 | 5 |
Na2SbAsCO7 (mp-771166) | 0.2554 | 0.009 | 5 |
Li12Mn3CrP4(CO7)4 (mp-767734) | 0.5541 | 0.060 | 6 |
Li12Mn3FeP4(CO7)4 (mp-767262) | 0.5622 | 0.050 | 6 |
Li6MnCrP2(CO7)2 (mp-767287) | 0.5557 | 0.066 | 6 |
Li6MnFeP2(CO7)2 (mp-767285) | 0.5635 | 0.047 | 6 |
NaLiMnPCO7 (mp-763833) | 0.5417 | 0.001 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Sb P C O |
Final Energy/Atom-6.5188 eV |
Corrected Energy-166.2823 eV
-166.2823 eV = -156.4503 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)