Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.100 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.035 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg3O4 + O2 + La2O3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3c [161] |
HallR 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 213.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 121.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 274.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 213.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 213.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 335.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 335.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 91.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 274.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 243.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 335.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 141.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 213.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 274.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 243.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 365.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 152.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 30.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 121.8 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 87.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 121.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 30.5 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 213.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 213.2 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 274.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 121.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 91.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 213.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 274.2 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 261.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 213.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 91.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 274.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 141.6 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 245.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 365.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 274.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 243.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 365.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 335.1 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 365.5 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 91.4 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 245.3 |
LiTaO3 (mp-3666) | <1 0 0> | <1 1 0> | 141.6 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 121.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 91.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 30.5 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 152.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 81.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 152.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TlNiO3 (mp-998845) | 0.2078 | 0.102 | 3 |
CaTcO3 (mp-998543) | 0.3339 | 0.029 | 3 |
MnTlO3 (mp-769883) | 0.4939 | 0.062 | 3 |
CuAsO3 (mp-776320) | 0.4960 | 0.092 | 3 |
AgSbO3 (mp-545999) | 0.5106 | 0.000 | 3 |
CaLa2CrO6 (mvc-13419) | 0.3541 | 0.063 | 4 |
CaLa2SnO6 (mvc-13402) | 0.2967 | 0.044 | 4 |
CaLa2MoO6 (mvc-11726) | 0.3308 | 0.129 | 4 |
CaLa2WO6 (mvc-15479) | 0.3324 | 0.198 | 4 |
CaLa2TiO6 (mvc-13624) | 0.3574 | 0.063 | 4 |
Pb2O3 (mp-20078) | 0.5080 | 0.009 | 2 |
PtO2 (mp-1285) | 0.4625 | 0.000 | 2 |
CeSe2 (mp-1080328) | 0.4858 | 0.121 | 2 |
CeSe2 (mp-1080851) | 0.5174 | 0.127 | 2 |
YbBr2 (mp-571232) | 0.5316 | 0.001 | 2 |
SrCoBiRuO6 (mp-743579) | 0.6121 | 0.086 | 5 |
Li4MnCr(WO6)2 (mp-761370) | 0.6108 | 0.071 | 5 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.5167 | 0.058 | 5 |
SrLaMnRuO6 (mp-39239) | 0.5688 | 0.093 | 5 |
LaMnZnFeO6 (mvc-8951) | 0.5876 | 0.178 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Ag O |
Final Energy/Atom-6.2010 eV |
Corrected Energy-66.2233 eV
-66.2233 eV = -62.0096 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)