Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.691 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.082 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO2 + LiMnF4 + MnF2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 339.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 193.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 48.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 163.7 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 169.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 193.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 266.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 363.4 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 218.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 169.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 48.5 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 171.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 145.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 218.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 145.4 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 72.7 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 241.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 290.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 315.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 315.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 163.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 339.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 218.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 363.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 363.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 266.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 363.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 245.5 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 266.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 363.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 363.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 290.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 193.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 218.1 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 218.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 193.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 266.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 218.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 266.5 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 266.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 245.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 339.2 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 266.5 |
GaSe (mp-1943) | <1 0 1> | <0 1 1> | 275.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 218.1 |
BN (mp-984) | <1 0 0> | <0 0 1> | 121.1 |
BN (mp-984) | <1 1 0> | <0 1 0> | 265.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 315.0 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 72.7 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 315.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnOF (mp-763936) | 0.3292 | 0.067 | 3 |
Mn12O7F17 (mp-764120) | 0.3284 | 0.081 | 3 |
Mn6O5F7 (mp-851262) | 0.3251 | 0.085 | 3 |
Mn6O5F7 (mp-850258) | 0.3182 | 0.729 | 3 |
Mn6O5F7 (mp-764625) | 0.3040 | 0.076 | 3 |
LiMn3(OF3)2 (mp-767125) | 0.3732 | 0.057 | 4 |
LiFe2OF5 (mp-777191) | 0.3933 | 0.057 | 4 |
LiGa(WO4)2 (mp-19695) | 0.3654 | 0.021 | 4 |
YTi(WO4)2 (mvc-785) | 0.3794 | 0.150 | 4 |
LiCo2OF5 (mp-849456) | 0.3839 | 0.300 | 4 |
TiO2 (mp-9173) | 0.5983 | 0.059 | 2 |
BiO2 (mvc-5760) | 0.5692 | 0.079 | 2 |
VO2 (mp-1094031) | 0.5705 | 0.018 | 2 |
VO2 (mp-715553) | 0.5508 | 0.072 | 2 |
TiO2 (mp-754769) | 0.5412 | 0.053 | 2 |
Li4VCr(WO6)2 (mp-761696) | 0.7466 | 0.050 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O F |
Final Energy/Atom-5.8269 eV |
Corrected Energy-226.0237 eV
-226.0237 eV = -209.7678 eV (uncorrected energy) - 13.4468 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)