Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.731 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaAlO3 |
Band Gap4.436 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 177.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 219.6 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 219.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 177.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 177.1 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 154.8 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 219.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 265.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 146.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 254.1 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 265.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 219.6 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 219.6 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 154.8 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 219.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 292.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 146.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 177.1 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 146.4 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 171.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 88.5 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 219.6 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 219.6 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 127.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 88.5 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 219.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 265.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 88.5 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 219.6 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 73.2 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 154.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 219.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 146.6 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 219.6 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 265.6 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 154.8 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 127.0 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 219.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 254.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 1> | 229.7 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 292.7 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 254.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 265.6 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 265.6 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 127.0 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 219.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 1> | 154.8 |
Au (mp-81) | <1 1 0> | <0 1 0> | 73.2 |
CdSe (mp-2691) | <1 0 0> | <1 0 1> | 154.8 |
WS2 (mp-224) | <1 0 0> | <0 1 1> | 229.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiBeH3 (mp-977148) | 0.2211 | 0.008 | 3 |
SrGeO3 (mp-17464) | 0.1924 | 0.000 | 3 |
CaSiO3 (mp-17552) | 0.3980 | 0.020 | 3 |
YAlO3 (mp-756705) | 0.3598 | 0.060 | 3 |
CaGeO3 (mp-776074) | 0.1845 | 0.030 | 3 |
Na2ZnP2O7 (mp-6491) | 0.6181 | 0.005 | 4 |
YSiNO2 (mp-559123) | 0.3897 | 0.008 | 4 |
K2MgV2O7 (mp-19459) | 0.6737 | 0.000 | 4 |
Na2CoP2O7 (mp-24887) | 0.6284 | 0.007 | 4 |
YSiNO2 (mp-559569) | 0.3910 | 0.005 | 4 |
Explore more synthesis descriptions for materials of composition LaAlO3.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Al O |
Final Energy/Atom-8.0149 eV |
Corrected Energy-253.0890 eV
-253.0890 eV = -240.4478 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)