Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.826 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.039 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYCl3 + BaCl2 |
Band Gap4.634 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 267.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 267.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 199.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 173.3 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 191.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 173.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 99.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 267.5 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 298.6 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 178.4 |
SiC (mp-8062) | <1 0 0> | <1 0 -1> | 191.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 199.1 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 199.1 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 173.3 |
GaSb (mp-1156) | <1 0 0> | <1 0 -1> | 191.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 298.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 298.6 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 298.6 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 99.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 298.6 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 199.1 |
PbSe (mp-2201) | <1 0 0> | <1 0 -1> | 191.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 267.5 |
ZnTe (mp-2176) | <1 0 0> | <1 0 -1> | 191.9 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 0> | 267.5 |
CdSe (mp-2691) | <1 0 0> | <1 0 -1> | 191.9 |
WS2 (mp-224) | <1 1 0> | <0 0 1> | 298.6 |
C (mp-48) | <1 0 0> | <0 1 0> | 267.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2ScCl7 (mp-573888) | 0.1576 | 0.026 | 3 |
Ba2LaCl7 (mp-773111) | 0.3602 | 0.076 | 3 |
Sr2RhF7 (mp-541114) | 0.4336 | 0.000 | 3 |
Ba2ScCl7 (mp-669476) | 0.3772 | 0.028 | 3 |
Ba2YBr7 (mp-768373) | 0.1902 | 0.035 | 3 |
Pr2SbO5F (mp-554138) | 0.7042 | 0.000 | 4 |
Rb2SbCl3F2 (mp-554605) | 0.6288 | 0.000 | 4 |
BaMgBiF7 (mvc-10353) | 0.7384 | 0.042 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Y_sv Cl |
Final Energy/Atom-4.7338 eV |
Corrected Energy-189.3527 eV
-189.3527 eV = -189.3527 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)