Final Magnetic Moment0.107 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.559 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.083 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi4O7 + Bi2O3 + Li3BiO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI23 [197] |
HallI 2 2 3 |
Point Group23 |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 178.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 206.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 103.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 146.1 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 146.1 |
C (mp-66) | <1 0 0> | <1 0 0> | 103.3 |
C (mp-66) | <1 1 0> | <1 1 0> | 146.1 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 178.9 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 146.1 |
InP (mp-20351) | <1 1 1> | <1 1 1> | 178.9 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 206.6 |
Au (mp-81) | <1 1 0> | <1 1 0> | 146.1 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <1 0 0> | 103.3 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 1 0> | 146.1 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <1 1 1> | 178.9 |
Al2O3 (mp-1143) | <0 0 1> | <1 1 1> | 178.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Er(Bi3O5)4 (mp-772790) | 0.3523 | 0.059 | 3 |
Bi12PbO20 (mp-667342) | 0.4105 | 0.017 | 3 |
Ho(Bi3O5)4 (mp-769405) | 0.3841 | 0.059 | 3 |
Zn(Bi3O5)4 (mp-28402) | 0.1665 | 0.062 | 3 |
Ga(Bi3O5)4 (mp-28632) | 0.4142 | 0.030 | 3 |
LiNiPO4 (mp-763061) | 0.6720 | 0.075 | 4 |
LiMnPO4 (mp-766735) | 0.6511 | 0.059 | 4 |
LiCoPO4 (mp-761780) | 0.6017 | 0.075 | 4 |
LiFePO4 (mp-762555) | 0.6686 | 0.083 | 4 |
Ba2Li3NbN4 (mp-567658) | 0.6653 | 0.014 | 4 |
Bi19O30 (mp-773884) | 0.6037 | 0.050 | 2 |
Bi2O3 (mp-759526) | 0.6362 | 0.034 | 2 |
Bi2O3 (mp-23262) | 0.7422 | 0.000 | 2 |
Si19Te8 (mp-31135) | 0.7022 | 0.035 | 2 |
Bi13O20 (mp-32597) | 0.3886 | 0.033 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Bi O |
Final Energy/Atom-5.6048 eV |
Corrected Energy-199.0049 eV
-199.0049 eV = -184.9591 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)