Final Magnetic Moment0.060 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.676 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiBiO3 + Bi4O7 + Li3BiO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmc21 [36] |
HallC 2c 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 117.8 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 178.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 117.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 175.0 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 175.0 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 178.4 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 186.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 258.7 |
BN (mp-984) | <0 0 1> | <0 1 0> | 235.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 1> | 178.4 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 134.0 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 258.7 |
SiC (mp-7631) | <1 0 0> | <1 0 1> | 186.2 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 1> | 178.4 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 117.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 235.7 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 1 0> | 117.8 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 175.0 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 258.7 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 258.7 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 1> | 186.2 |
C (mp-48) | <1 0 1> | <1 0 0> | 258.7 |
Si (mp-149) | <1 0 0> | <0 1 0> | 117.8 |
ZrO2 (mp-2858) | <1 0 1> | <1 1 0> | 175.0 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 134.0 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 235.7 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 1> | 186.2 |
TiO2 (mp-390) | <0 0 1> | <1 1 0> | 175.0 |
CsI (mp-614603) | <1 1 0> | <0 1 1> | 178.4 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 1> | 186.2 |
ZnO (mp-2133) | <1 0 0> | <1 1 0> | 175.0 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 117.8 |
MgF2 (mp-1249) | <1 0 1> | <1 0 1> | 186.2 |
LiAlO2 (mp-3427) | <1 0 1> | <1 1 0> | 175.0 |
SrTiO3 (mp-4651) | <1 0 0> | <0 1 1> | 178.4 |
GaTe (mp-542812) | <1 0 0> | <0 0 1> | 134.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgFeO3 (mp-762508) | 0.6252 | 0.131 | 3 |
LiFeF3 (mp-775778) | 0.6275 | 0.096 | 3 |
Li2VF4 (mp-765541) | 0.5469 | 0.065 | 3 |
Li2FeF4 (mp-853234) | 0.5892 | 0.095 | 3 |
NaTi4O8 (mp-757433) | 0.6042 | 0.023 | 3 |
Li4Fe3OF8 (mp-850180) | 0.5385 | 0.108 | 4 |
Li2MnOF3 (mp-765036) | 0.6020 | 0.091 | 4 |
Li2Mn3O4F3 (mp-767162) | 0.6708 | 0.381 | 4 |
Li4Co7(OF7)2 (mp-765676) | 0.5842 | 0.061 | 4 |
HoZn(BiO3)2 (mvc-9931) | 0.6707 | 0.089 | 4 |
V3O5 (mp-714914) | 0.7315 | 0.004 | 2 |
Mn2O3 (mp-779818) | 0.7257 | 0.079 | 2 |
Fe3O4 (mp-541907) | 0.6546 | 0.164 | 2 |
Fe3O4 (mp-715310) | 0.7202 | 0.164 | 2 |
Li4FeTe(WO6)2 (mp-771716) | 0.7302 | 0.070 | 5 |
Li4MnNb2WO12 (mp-771475) | 0.6800 | 0.047 | 5 |
Li4CrTe2WO12 (mp-775509) | 0.7292 | 0.109 | 5 |
Li4FeTe2WO12 (mp-775176) | 0.7280 | 0.073 | 5 |
LiTi3Nb(CuO4)3 (mp-849772) | 0.7178 | 0.081 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Bi O |
Final Energy/Atom-5.2894 eV |
Corrected Energy-284.1320 eV
-284.1320 eV = -264.4679 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)