material

Al(CrB)2

ID:

mp-7692

DOI:

10.17188/1298665


Tags: Aluminium chromium boride (1/2/2) Chromium aluminium boride (2/1/2)

Material Details

Final Magnetic Moment
0.040 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.466 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.33 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmmm [65]
Hall
-C 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 20083 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SrTiO3 (mp-4651) <1 1 0> <0 1 0> 0.006 249.3
GaSb (mp-1156) <1 0 0> <0 1 0> 0.007 77.4
SrTiO3 (mp-4651) <0 0 1> <0 1 0> 0.010 154.7
CdSe (mp-2691) <1 0 0> <0 1 0> 0.010 77.4
YAlO3 (mp-3792) <1 1 0> <0 1 0> 0.010 111.8
PbSe (mp-2201) <1 0 0> <0 1 0> 0.012 77.4
YAlO3 (mp-3792) <0 1 1> <0 1 0> 0.014 240.7
TePb (mp-19717) <1 0 0> <0 1 0> 0.016 43.0
Ag (mp-124) <1 0 0> <0 1 0> 0.051 17.2
TiO2 (mp-2657) <0 0 1> <0 1 0> 0.051 43.0
SiC (mp-8062) <1 0 0> <0 1 0> 0.065 77.4
Ni (mp-23) <1 0 0> <0 1 0> 0.074 111.8
CsI (mp-614603) <1 0 0> <0 1 0> 0.074 249.3
SrTiO3 (mp-4651) <1 0 1> <1 0 1> 0.087 320.5
SiC (mp-11714) <1 0 1> <0 1 0> 0.088 292.3
ZnTe (mp-2176) <1 0 0> <0 1 0> 0.113 77.4
GaTe (mp-542812) <1 0 1> <0 1 0> 0.120 292.3
Cu (mp-30) <1 1 0> <0 1 0> 0.122 128.9
LiAlO2 (mp-3427) <1 1 1> <0 1 0> 0.122 214.9
Cu (mp-30) <1 1 1> <0 1 0> 0.123 180.5
Te2Mo (mp-602) <1 0 0> <0 1 0> 0.129 275.1
InAs (mp-20305) <1 0 0> <0 1 0> 0.135 77.4
TiO2 (mp-2657) <1 1 1> <0 1 0> 0.135 232.1
SiC (mp-11714) <1 1 0> <0 0 1> 0.139 161.6
Au (mp-81) <1 0 0> <0 1 0> 0.140 17.2
C (mp-48) <1 1 0> <0 1 0> 0.142 266.5
CsI (mp-614603) <1 1 0> <0 0 1> 0.155 258.6
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.166 97.0
ZrO2 (mp-2858) <0 0 1> <0 1 0> 0.173 111.8
BN (mp-984) <1 1 0> <0 1 0> 0.181 232.1
AlN (mp-661) <1 1 0> <0 0 1> 0.184 161.6
Te2W (mp-22693) <0 1 0> <0 1 0> 0.197 163.3
NdGaO3 (mp-3196) <0 1 1> <1 0 1> 0.201 320.5
C (mp-48) <0 0 1> <0 1 0> 0.205 94.6
DyScO3 (mp-31120) <0 1 1> <0 1 0> 0.210 318.1
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.219 193.9
LaF3 (mp-905) <1 0 0> <0 1 0> 0.234 214.9
DyScO3 (mp-31120) <1 1 0> <0 1 0> 0.235 249.3
KP(HO2)2 (mp-23959) <0 0 1> <0 1 0> 0.275 223.5
Fe2O3 (mp-24972) <0 0 1> <0 1 0> 0.276 180.5
Ag (mp-124) <1 1 1> <0 1 0> 0.279 206.3
GdScO3 (mp-5690) <1 0 1> <0 1 0> 0.280 171.9
ZrO2 (mp-2858) <1 0 -1> <0 1 0> 0.281 283.7
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 1 0> 0.283 111.8
TeO2 (mp-2125) <1 1 0> <0 1 0> 0.285 292.3
GdScO3 (mp-5690) <0 0 1> <0 1 0> 0.297 223.5
NdGaO3 (mp-3196) <1 1 0> <0 1 0> 0.312 249.3
Al2O3 (mp-1143) <1 0 1> <1 1 1> 0.316 326.1
TiO2 (mp-2657) <1 1 0> <0 1 0> 0.317 77.4
PbS (mp-21276) <1 1 0> <0 1 0> 0.318 300.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
447 114 117 0 0 0
114 421 101 0 0 0
117 101 518 0 0 0
0 0 0 160 0 0
0 0 0 0 211 0
0 0 0 0 0 158
Compliance Tensor Sij (10-12Pa-1)
2.5 -0.6 -0.5 0 0 0
-0.6 2.6 -0.4 0 0 0
-0.5 -0.4 2.1 0 0 0
0 0 0 6.3 0 0
0 0 0 0 4.7 0
0 0 0 0 0 6.3
Shear Modulus GV
176 GPa
Bulk Modulus KV
228 GPa
Shear Modulus GR
173 GPa
Bulk Modulus KR
226 GPa
Shear Modulus GVRH
175 GPa
Bulk Modulus KVRH
227 GPa
Elastic Anisotropy
0.08
Poisson's Ratio
0.19

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Al(FeB)2 (mp-997634) 0.1215 0.000 3
Mn2AlB2 (mp-1001965) 0.1907 0.000 3
Al(FeB)2 (mp-3805) 0.1292 0.000 3
Mn2AlB2 (mp-7892) 0.1879 0.000 3
Ho2Ni2Pb (mp-3398) 0.3693 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al Cr_pv B
Final Energy/Atom
-7.7478 eV
Corrected Energy
-38.7392 eV
-38.7392 eV = -38.7392 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 251805
  • 236647
  • 20083
Submitted by
User remarks:
  • Chromium aluminium boride (2/1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)