Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.182 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.046 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.82 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CuP2O7 + CuO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 237.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 237.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 285.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 237.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 248.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 159.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 333.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 190.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 285.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 333.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 114.6 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 242.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 333.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 114.6 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 333.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 333.1 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 237.9 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 190.3 |
C (mp-66) | <1 0 0> | <0 0 1> | 333.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 333.1 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 237.9 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 159.9 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 333.1 |
InSb (mp-20012) | <1 0 0> | <0 1 0> | 222.9 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 190.3 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 142.7 |
NdGaO3 (mp-3196) | <1 0 1> | <1 1 0> | 159.9 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 190.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 333.1 |
GaSe (mp-1943) | <1 1 0> | <0 1 1> | 121.2 |
BN (mp-984) | <1 0 1> | <1 1 0> | 159.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 333.1 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 222.9 |
TeO2 (mp-2125) | <0 1 1> | <0 1 0> | 222.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 285.5 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 237.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 237.9 |
CdWO4 (mp-19387) | <1 1 0> | <0 0 1> | 237.9 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 190.3 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 333.1 |
TiO2 (mp-390) | <1 1 0> | <1 1 0> | 159.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 190.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 229.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 142.7 |
C (mp-66) | <1 1 1> | <0 0 1> | 333.1 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 333.1 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 190.3 |
MgF2 (mp-1249) | <1 1 1> | <0 1 1> | 121.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 159.9 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 333.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr4(PO4)3 (mp-504357) | 0.6497 | 0.784 | 3 |
V2Cu3O8 (mp-504747) | 0.6433 | 0.012 | 3 |
CuSiO3 (mp-556982) | 0.6178 | 0.054 | 3 |
Cu5(Si2O7)2 (mp-25205) | 0.6450 | 0.115 | 3 |
Cr4(PO4)3 (mp-773959) | 0.6500 | 0.784 | 3 |
LiCrPO4 (mp-540381) | 0.2369 | 0.033 | 4 |
Na2Cu5(Si2O7)2 (mp-573024) | 0.5705 | 0.062 | 4 |
Li2CoP2O7 (mp-761665) | 0.5510 | 0.118 | 4 |
TlCuAsO4 (mp-541202) | 0.5330 | 0.000 | 4 |
Cu3B4Pb2O11 (mp-560136) | 0.5655 | 0.030 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Cu_pv P O |
Final Energy/Atom-6.2400 eV |
Corrected Energy-185.9569 eV
-185.9569 eV = -174.7202 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)