Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.492 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.33 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCa4Ta2O9 |
Band Gap4.501 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3c1 [165] |
Hall-P 3 2"c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 333.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 333.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 166.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 194.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 250.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 306.0 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 333.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 166.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 83.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 84.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 139.1 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 333.8 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 361.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 222.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 361.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 222.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 194.7 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 194.7 |
C (mp-66) | <1 0 0> | <0 0 1> | 250.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 139.1 |
C (mp-66) | <1 1 1> | <0 0 1> | 83.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 166.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 306.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 111.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.8 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 166.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 222.6 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 55.6 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 222.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 55.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 111.3 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 267.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 83.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 166.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 27.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 111.3 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 306.0 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 333.8 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 361.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 333.8 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 333.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 194.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 306.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 361.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 333.8 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 222.6 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 222.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn4Nb2O9 (mp-640040) | 0.2703 | 0.000 | 3 |
Sr4Ta2O9 (mp-769268) | 0.2865 | 0.032 | 3 |
Ta2Mn4O9 (mp-31905) | 0.2544 | 0.000 | 3 |
TiMnO3 (mp-19376) | 0.2982 | 0.036 | 3 |
TiMnO3 (mp-819044) | 0.3012 | 0.036 | 3 |
Li3V4SnO12 (mp-775037) | 0.3858 | 0.069 | 4 |
Li3Nb4NiO12 (mp-772009) | 0.3419 | 0.089 | 4 |
Li3Nb4FeO12 (mp-771984) | 0.4082 | 0.030 | 4 |
TiFe(BiO3)2 (mp-560185) | 0.2985 | 0.015 | 4 |
Li3MnV4O12 (mp-771987) | 0.3935 | 0.285 | 4 |
Y2O3 (mp-775906) | 0.4685 | 0.063 | 2 |
Y2O3 (mp-754759) | 0.4611 | 0.051 | 2 |
Fe2O3 (mp-542309) | 0.4709 | 0.131 | 2 |
Al2O3 (mp-1938) | 0.4694 | 0.093 | 2 |
In2O3 (mp-22323) | 0.4681 | 0.029 | 2 |
Li4Fe2TeWO12 (mp-768021) | 0.5922 | 0.083 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.6654 | 0.081 | 5 |
Li4MnV2WO12 (mp-773239) | 0.6586 | 0.088 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.6718 | 0.054 | 5 |
Li4V2CrTeO12 (mp-775632) | 0.6387 | 0.181 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Ta_pv O |
Final Energy/Atom-8.1540 eV |
Corrected Energy-257.2627 eV
-257.2627 eV = -244.6215 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)