Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.198 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.045 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi2O3 + Dy2O3 |
Band Gap2.095 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 267.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 89.1 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 267.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 89.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 267.4 |
BN (mp-984) | <1 1 0> | <0 0 1> | 267.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 267.4 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 267.4 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 267.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 89.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 267.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 267.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 267.4 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 89.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 89.1 |
TiO2 (mp-390) | <1 0 0> | <1 0 1> | 147.1 |
TiO2 (mp-390) | <1 0 1> | <1 0 0> | 117.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 267.4 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 267.4 |
Cu (mp-30) | <1 1 0> | <1 0 1> | 147.1 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 89.1 |
C (mp-66) | <1 1 1> | <0 0 1> | 89.1 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 267.4 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 267.4 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 267.4 |
BaTiO3 (mp-5986) | <1 1 1> | <1 0 0> | 117.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 267.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 89.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3CuF6 (mp-753063) | 0.1991 | 0.002 | 3 |
Li3VF6 (mp-777528) | 0.2062 | 0.052 | 3 |
Er(BiO2)3 (mp-754989) | 0.0441 | 0.042 | 3 |
Lu(BiO2)3 (mp-754693) | 0.1177 | 0.038 | 3 |
Y(BiO2)3 (mp-754107) | 0.0237 | 0.044 | 3 |
Mg2CoWO6 (mvc-5853) | 0.3683 | 0.017 | 4 |
Mg2VWO6 (mvc-5881) | 0.3522 | 0.023 | 4 |
Mg2MoWO6 (mvc-5910) | 0.3619 | 0.033 | 4 |
Mg2FeWO6 (mvc-5956) | 0.3664 | 0.005 | 4 |
InNi2SbO6 (mp-1078367) | 0.3696 | 0.000 | 4 |
Fe2O3 (mp-777192) | 0.3345 | 0.123 | 2 |
Fe2O3 (mp-715572) | 0.3723 | 0.077 | 2 |
Al2O3 (mp-776475) | 0.3633 | 0.030 | 2 |
Al2O3 (mp-776490) | 0.3913 | 0.048 | 2 |
V2O3 (mp-849288) | 0.3799 | 0.031 | 2 |
Li4Fe2TeWO12 (mp-768021) | 0.4913 | 0.083 | 5 |
CaLaTaCrO6 (mvc-10008) | 0.6229 | 0.035 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.6165 | 0.080 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.5835 | 0.058 | 5 |
Li4V2CrTeO12 (mp-775632) | 0.5849 | 0.104 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 Bi O |
Final Energy/Atom-6.3733 eV |
Corrected Energy-135.8938 eV
-135.8938 eV = -127.4663 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|