Final Magnetic Moment18.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.595 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.74 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa2V2O7 + V2O3 |
Band Gap1.017 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 1> | <1 0 -1> | 271.0 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 184.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 173.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 260.3 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 260.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 271.0 |
Te2Mo (mp-602) | <1 1 0> | <1 0 -1> | 90.3 |
Te2Mo (mp-602) | <1 1 1> | <1 0 1> | 184.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 173.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 86.8 |
GaSe (mp-1943) | <1 0 0> | <1 0 -1> | 271.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 260.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 233.1 |
SiC (mp-7631) | <1 0 0> | <1 0 -1> | 90.3 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 180.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 260.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 116.5 |
Mg (mp-153) | <1 0 0> | <1 0 1> | 184.6 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 260.3 |
PbS (mp-21276) | <1 0 0> | <1 0 -1> | 180.6 |
InP (mp-20351) | <1 0 0> | <1 0 -1> | 180.6 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 260.3 |
PbSe (mp-2201) | <1 1 1> | <1 0 -1> | 271.0 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 260.3 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 -1> | 271.0 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 -1> | 90.3 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 260.3 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 260.3 |
CdSe (mp-2691) | <1 1 1> | <1 0 -1> | 271.0 |
Au (mp-81) | <1 1 0> | <1 0 0> | 173.5 |
WSe2 (mp-1821) | <0 0 1> | <1 0 -1> | 271.0 |
C (mp-48) | <1 0 0> | <1 0 -1> | 271.0 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 260.3 |
CdWO4 (mp-19387) | <0 0 1> | <1 0 -1> | 90.3 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 86.8 |
SiC (mp-8062) | <1 1 0> | <1 0 -1> | 271.0 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 86.8 |
ZnO (mp-2133) | <1 0 1> | <1 0 -1> | 180.6 |
MgF2 (mp-1249) | <1 0 1> | <1 0 -1> | 180.6 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 260.3 |
GaSb (mp-1156) | <1 1 1> | <1 0 -1> | 271.0 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 260.3 |
ZnTe (mp-2176) | <1 1 0> | <1 0 0> | 260.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Ba_sv V_pv O |
Final Energy/Atom-7.8845 eV |
Corrected Energy-499.0522 eV
-499.0522 eV = -441.5343 eV (uncorrected energy) - 33.6400 eV (MP Advanced Correction) - 23.8779 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)