Final Magnetic Moment16.979 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.380 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiO2 + Li19Ni23O42 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
InAs (mp-20305) | <1 1 0> | <1 1 0> | 109.5 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 205.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 184.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 227.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 184.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 -1> | 145.3 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 227.1 |
CdS (mp-672) | <1 0 1> | <1 0 -1> | 302.8 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 257.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 184.0 |
LiF (mp-1138) | <1 1 1> | <0 1 -1> | 145.3 |
Te2W (mp-22693) | <0 0 1> | <1 -1 1> | 198.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 321.3 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 213.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 306.6 |
AlN (mp-661) | <1 0 1> | <1 -1 0> | 307.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 306.6 |
AlN (mp-661) | <1 1 1> | <1 -1 -1> | 291.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 205.0 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 102.5 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 218.9 |
Ag (mp-124) | <1 1 1> | <0 1 -1> | 145.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 184.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 102.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 109.5 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 205.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 -1> | 217.9 |
GaN (mp-804) | <0 0 1> | <1 -1 0> | 153.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 184.0 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 257.0 |
GaN (mp-804) | <1 1 1> | <1 0 -1> | 151.4 |
BN (mp-984) | <0 0 1> | <1 1 0> | 109.5 |
BN (mp-984) | <1 0 0> | <1 0 1> | 213.6 |
BN (mp-984) | <1 0 1> | <1 1 -1> | 101.5 |
BN (mp-984) | <1 1 0> | <0 1 1> | 102.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 245.3 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 217.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 227.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 -1> | 72.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 -1> | 217.9 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 205.0 |
LiNbO3 (mp-3731) | <1 0 0> | <1 -1 1> | 298.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 306.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 184.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 -1> | 291.3 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 321.3 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 227.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 184.0 |
Al (mp-134) | <1 1 1> | <0 1 -1> | 145.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 257.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4Ni5O9 (mp-767950) | 0.0873 | 0.051 | 3 |
Li19Ni23O42 (mp-698842) | 0.1188 | 0.000 | 3 |
Li5Ni7O12 (mp-771626) | 0.1265 | 0.015 | 3 |
Li13Ni15O28 (mp-761369) | 0.1017 | 0.006 | 3 |
Li7Ni5O12 (mp-761436) | 0.1457 | 0.021 | 3 |
Li5Co5(NiO6)2 (mp-766793) | 0.1317 | 0.230 | 4 |
Li5Mn2Ni3O10 (mp-771234) | 0.1237 | 0.015 | 4 |
Li4Ni3O6F (mp-764986) | 0.1365 | 0.062 | 4 |
Li5Mn5(FeO6)2 (mp-765929) | 0.1123 | 0.032 | 4 |
Li4FeNi3O8 (mp-765712) | 0.1238 | 0.179 | 4 |
Te2Au (mp-1662) | 0.3734 | 0.018 | 2 |
NaTe3 (mp-28478) | 0.3846 | 0.000 | 2 |
LiTe3 (mp-27466) | 0.3067 | 0.009 | 2 |
Sb2Te3 (mp-1080789) | 0.4136 | 0.129 | 2 |
Te2Au (mp-567525) | 0.3866 | 0.018 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.4210 | 0.139 | 5 |
Hg (mp-982872) | 0.6279 | 0.020 | 1 |
Sb (mp-632286) | 0.4587 | 0.059 | 1 |
Bi (mp-23152) | 0.6075 | 0.000 | 1 |
Te (mp-570459) | 0.4519 | 0.044 | 1 |
Te (mp-105) | 0.5270 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv O |
Final Energy/Atom-4.9146 eV |
Corrected Energy-327.3418 eV
-327.3418 eV = -275.2176 eV (uncorrected energy) - 32.4600 eV (MP Advanced Correction) - 19.6641 eV (MP Anion Correction)
|