Final Magnetic Moment15.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.711 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.091 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiTiCrO4 + LiMnCrO4 + TiO2 |
Band Gap0.731 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbam [55] |
Hall-P 2 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 146.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 352.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 219.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 189.5 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 292.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 324.9 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 219.2 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 311.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 189.5 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 219.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 81.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 297.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 162.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 324.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 292.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 324.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 352.0 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 219.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 146.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 81.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 292.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 243.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 352.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 216.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 216.6 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 146.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 243.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 297.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 243.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 297.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 243.7 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 243.7 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 243.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 243.7 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 155.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 216.6 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 146.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 297.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 108.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 189.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 292.3 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 311.7 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 216.6 |
BN (mp-984) | <0 0 1> | <0 1 0> | 219.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 216.6 |
BN (mp-984) | <1 0 1> | <0 1 0> | 219.2 |
BN (mp-984) | <1 1 0> | <0 1 1> | 233.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 189.5 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 243.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 243.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca(NiO2)2 (mvc-12644) | 0.4802 | 0.156 | 3 |
Li4(FeO2)9 (mp-771396) | 0.3059 | 0.099 | 3 |
Ca(CuO2)2 (mvc-7250) | 0.5101 | 0.284 | 3 |
Mg(FeO2)4 (mvc-12639) | 0.5437 | 0.152 | 3 |
LiMn2O4 (mp-1016095) | 0.5308 | 0.053 | 3 |
Li4V5(Fe2O9)2 (mp-775660) | 0.2592 | 0.082 | 4 |
Li4Ti4Mn5O18 (mp-769512) | 0.3034 | 0.061 | 4 |
Li4Ti2V7O18 (mp-769491) | 0.3680 | 0.088 | 4 |
Li4Ti4V5O18 (mp-769487) | 0.3705 | 0.081 | 4 |
Li4Ti4Cr5O18 (mp-861696) | 0.3621 | 0.095 | 4 |
In6Se7 (mp-567596) | 0.7029 | 0.043 | 2 |
In6S7 (mp-555853) | 0.6050 | 0.012 | 2 |
Li4Ti4V4CoO18 (mp-769478) | 0.2610 | 0.076 | 5 |
Li4Ti4Cr(Fe2O9)2 (mp-769457) | 0.2655 | 0.088 | 5 |
Li4Ti4Mn(Fe2O9)2 (mp-769443) | 0.2503 | 0.082 | 5 |
Li4Ti4VCr4O18 (mp-775391) | 0.1022 | 0.085 | 5 |
Li4TiV4Cr4O18 (mp-767927) | 0.2767 | 0.081 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Mn_pv Cr_pv O |
Final Energy/Atom-7.6589 eV |
Corrected Energy-519.5978 eV
-519.5978 eV = -474.8497 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 19.4657 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)