Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.214 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.222 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 149.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 149.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 149.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 239.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 29.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 268.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 -1> | 221.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 89.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 268.8 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 110.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 114.6 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 125.7 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 159.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 110.7 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 239.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 89.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 149.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 328.6 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 114.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 149.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 125.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 110.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 268.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 149.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 268.8 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 328.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 229.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 149.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 358.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 328.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 149.4 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 268.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 149.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 59.7 |
BN (mp-984) | <1 1 0> | <1 1 1> | 167.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 89.6 |
MoS2 (mp-1434) | <1 1 0> | <1 0 0> | 114.6 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 149.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 149.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 179.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 110.7 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 328.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 179.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 89.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 119.5 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 -1> | 110.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 -1> | 221.3 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 268.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba3Zr2S7 (mp-8570) | 0.5994 | 0.000 | 3 |
Ba4Pb3O10 (mp-752906) | 0.6303 | 0.014 | 3 |
Sr4Ru3O10 (mp-680680) | 0.6209 | 0.001 | 3 |
Sr4Hf3O10 (mp-779001) | 0.5989 | 0.012 | 3 |
Sr3Ru2O7 (mp-559909) | 0.5574 | 0.000 | 3 |
SrEu2Fe2O7 (mp-603128) | 0.6238 | 0.000 | 4 |
La3Ti2N3O4 (mp-754845) | 0.6004 | 0.061 | 4 |
SrTaNO2 (mp-755441) | 0.6270 | 0.003 | 4 |
BaEu2Mn2O7 (mp-579071) | 0.4585 | 0.000 | 4 |
BaNd2Mn2O7 (mp-18861) | 0.5269 | 0.002 | 4 |
Sr9NdFe5(MoO6)5 (mp-698711) | 0.6600 | 0.009 | 5 |
Sr4La4Mn7CuO24 (mp-698710) | 0.6305 | 0.008 | 5 |
Sr5La5Mn9CuO30 (mp-698602) | 0.6311 | 0.006 | 5 |
Sr7SmFe4(MoO6)4 (mp-694963) | 0.5815 | 0.045 | 5 |
Sr11LaFe6(MoO6)6 (mp-735565) | 0.6306 | 0.006 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv La Mn_pv O |
Final Energy/Atom-7.7029 eV |
Corrected Energy-396.1262 eV
-396.1262 eV = -369.7386 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|