Final Magnetic Moment2.994 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.262 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa2MnPCO7 |
Band Gap0.938 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 279.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 228.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 225.9 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 228.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 152.2 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 150.6 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 240.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 76.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 225.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 228.2 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 301.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 225.9 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 304.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 209.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 279.7 |
BN (mp-984) | <1 0 1> | <1 -1 0> | 184.0 |
BN (mp-984) | <1 1 0> | <1 -1 0> | 275.9 |
BN (mp-984) | <1 1 1> | <0 1 0> | 301.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 209.8 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 150.6 |
Al (mp-134) | <1 1 0> | <0 1 0> | 225.9 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 304.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 103.6 |
LiGaO2 (mp-5854) | <1 1 1> | <1 -1 0> | 275.9 |
TeO2 (mp-2125) | <0 1 0> | <1 -1 0> | 275.9 |
TeO2 (mp-2125) | <1 0 0> | <1 -1 0> | 275.9 |
LaF3 (mp-905) | <1 1 1> | <0 0 1> | 209.8 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 152.2 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 152.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 304.3 |
MgO (mp-1265) | <1 1 0> | <1 -1 1> | 232.1 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 76.1 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 240.5 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 228.2 |
TiO2 (mp-2657) | <1 1 0> | <1 -1 0> | 275.9 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 228.2 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 304.3 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 279.7 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 279.7 |
SiC (mp-11714) | <1 1 1> | <0 0 1> | 209.8 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 150.6 |
MoSe2 (mp-1634) | <0 0 1> | <1 1 0> | 240.5 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 209.8 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 304.3 |
Au (mp-81) | <1 1 1> | <0 0 1> | 209.8 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 76.1 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 150.6 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 152.2 |
C (mp-48) | <1 0 1> | <0 0 1> | 139.9 |
C (mp-48) | <1 1 0> | <0 1 0> | 301.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3Ca(BO2)5 (mp-542719) | 0.7485 | 0.000 | 4 |
YbCu2(MoO4)3 (mp-565220) | 0.7090 | 0.046 | 4 |
Na2NiPCO7 (mp-768089) | 0.2574 | 0.060 | 5 |
Na2NiPCO7 (mp-775744) | 0.2378 | 0.049 | 5 |
Na2MnPCO7 (mp-868618) | 0.0586 | 0.037 | 5 |
Na2MnPCO7 (mp-775643) | 0.2548 | 0.000 | 5 |
Na2MnPCO7 (mp-768085) | 0.0349 | 0.117 | 5 |
Na5LiNi2P2(CO7)2 (mp-770324) | 0.5786 | 0.009 | 6 |
Na2LiFePCO7 (mp-773940) | 0.5483 | 0.099 | 6 |
Na2LiFePCO7 (mp-773705) | 0.5627 | 0.138 | 6 |
NaLi2FePCO7 (mp-773689) | 0.6162 | 0.150 | 6 |
Na3Li3Fe2P2(CO7)2 (mp-773524) | 0.5888 | 0.148 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Mn_pv P C O |
Final Energy/Atom-6.8007 eV |
Corrected Energy-352.8210 eV
-352.8210 eV = -326.4335 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)