Final Magnetic Moment9.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.298 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.018 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3FePCO7 + Na2FePCO7 |
Band Gap0.957 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KCl (mp-23193) | <1 1 1> | <0 1 0> | 283.0 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 283.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 68.6 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 117.1 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 119.6 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 283.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 283.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 277.8 |
GaSe (mp-1943) | <1 1 0> | <1 0 1> | 119.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 283.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 283.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 68.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 205.9 |
C (mp-66) | <1 1 1> | <0 1 0> | 283.0 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 117.1 |
KP(HO2)2 (mp-23959) | <1 0 1> | <0 0 1> | 137.3 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 233.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 137.3 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 208.3 |
SiC (mp-11714) | <1 1 0> | <1 0 -1> | 206.9 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 233.3 |
PbSe (mp-2201) | <1 1 1> | <0 1 0> | 283.0 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 205.9 |
MoSe2 (mp-1634) | <1 0 1> | <0 0 1> | 205.9 |
CdSe (mp-2691) | <1 1 1> | <0 1 0> | 283.0 |
C (mp-48) | <0 0 1> | <1 0 0> | 277.8 |
WSe2 (mp-1821) | <1 0 1> | <0 0 1> | 205.9 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 283.0 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 283.0 |
CaCO3 (mp-3953) | <0 0 1> | <0 1 0> | 283.0 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 283.0 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 283.0 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 0> | 283.0 |
YAlO3 (mp-3792) | <0 1 1> | <0 1 0> | 94.3 |
YAlO3 (mp-3792) | <1 1 0> | <0 1 0> | 283.0 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 274.5 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 208.3 |
TiO2 (mp-390) | <1 1 1> | <1 0 0> | 208.3 |
MgF2 (mp-1249) | <1 1 1> | <1 0 1> | 119.6 |
ZnO (mp-2133) | <1 0 0> | <0 0 1> | 68.6 |
ZnO (mp-2133) | <1 1 0> | <1 1 1> | 152.3 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 205.9 |
GaSb (mp-1156) | <1 1 1> | <0 1 0> | 283.0 |
Fe2O3 (mp-24972) | <1 0 0> | <0 1 0> | 283.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na5Fe2P2(CO7)2 (mp-769488) | 0.1648 | 0.010 | 5 |
Na5Fe2P2(CO7)2 (mp-769456) | 0.0671 | 0.017 | 5 |
Na5Fe2P2(CO7)2 (mp-770837) | 0.1807 | 0.010 | 5 |
Na5Fe2P2(CO7)2 (mp-770394) | 0.1602 | 0.010 | 5 |
Na5Fe2P2(CO7)2 (mp-767966) | 0.0805 | 0.014 | 5 |
Na5LiFe2P2(CO7)2 (mp-773528) | 0.3277 | 0.013 | 6 |
Na5LiFe2P2(CO7)2 (mp-773523) | 0.3246 | 0.014 | 6 |
Na5LiFe2P2(CO7)2 (mp-770144) | 0.3159 | 0.010 | 6 |
Na5LiFe2P2(CO7)2 (mp-769718) | 0.3069 | 0.010 | 6 |
Na5LiFe2P2(CO7)2 (mp-773414) | 0.3182 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Na_pv Fe_pv P C O |
Final Energy/Atom-6.5703 eV |
Corrected Energy-359.1136 eV
-359.1136 eV = -328.5175 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)