Final Magnetic Moment4.995 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.416 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.060 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiO2 + Mg3NiO4 + Li(NiO2)2 + Li2NiO3 |
Band Gap0.070 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2 [5] |
HallC 2y |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 221.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 108.8 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 326.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 286.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 233.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 295.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 113.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 326.5 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 245.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 233.2 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 143.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 113.6 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 295.6 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 186.6 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 233.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 229.2 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 295.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 326.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 286.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 326.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 186.6 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 233.2 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 326.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 171.9 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 139.9 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 221.7 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 326.5 |
BN (mp-984) | <0 0 1> | <1 0 0> | 286.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 233.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 326.5 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 326.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 286.5 |
MoS2 (mp-1434) | <0 0 1> | <1 1 -1> | 236.8 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 143.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 326.5 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 245.6 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 326.5 |
Al (mp-134) | <1 0 0> | <0 1 0> | 233.2 |
Al (mp-134) | <1 1 0> | <1 0 0> | 286.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 113.6 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 171.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 139.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 139.9 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 139.9 |
LiGaO2 (mp-5854) | <0 1 0> | <1 1 0> | 221.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 171.9 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 0> | 221.7 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 186.6 |
CdTe (mp-406) | <1 1 1> | <0 1 0> | 233.2 |
MgO (mp-1265) | <1 0 0> | <1 1 -1> | 236.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li14Co13O28 (mp-777836) | 0.2502 | 0.152 | 3 |
Li7Mn4O12 (mp-764763) | 0.2463 | 0.042 | 3 |
Li4Ni7O12 (mp-997521) | 0.2509 | 0.060 | 3 |
Li9(NiO2)10 (mp-769454) | 0.2511 | 0.002 | 3 |
Li7(NiO2)8 (mp-690528) | 0.2198 | 0.019 | 3 |
Li4Ti2Fe5O12 (mp-762689) | 0.2607 | 0.429 | 4 |
Li4Mn5(NiO6)2 (mp-762589) | 0.2546 | 0.037 | 4 |
Li4V5Cr2O12 (mp-780923) | 0.2461 | 0.053 | 4 |
Li4Mn2Co5O12 (mp-774397) | 0.2302 | 0.555 | 4 |
Li7MgNi7O16 (mp-771050) | 0.1867 | 0.019 | 4 |
Fe10O11 (mp-764330) | 0.3331 | 0.057 | 2 |
Fe17O18 (mp-705424) | 0.2837 | 0.041 | 2 |
Fe21O23 (mp-706875) | 0.3437 | 0.055 | 2 |
Fe23O25 (mp-705553) | 0.3150 | 0.051 | 2 |
Fe10O11 (mp-705555) | 0.3680 | 0.046 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4304 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Mg_pv Ni_pv O |
Final Energy/Atom-4.9070 eV |
Corrected Energy-178.5014 eV
-178.5014 eV = -152.1168 eV (uncorrected energy) - 15.1480 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)