Final Magnetic Moment0.503 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.087 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.120 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi(CoO2)2 + LiCoO2 + TiO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm [6] |
HallP 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 301.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 212.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 126.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 228.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 283.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 141.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 141.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 203.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 141.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 329.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 279.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 203.0 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 301.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 253.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 253.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 141.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 279.1 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 279.1 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 253.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 101.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 141.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 76.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 177.6 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 150.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 279.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 212.7 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 279.1 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 203.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 177.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 329.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 329.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 329.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 177.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 253.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 228.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 279.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 279.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 283.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 304.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 329.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 76.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 212.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 101.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 50.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 225.9 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 1> | 225.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 279.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 329.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 50.8 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 101.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4(FeO2)9 (mp-771396) | 0.4176 | 0.121 | 3 |
Mg(BiO2)4 (mvc-2854) | 0.5282 | 0.147 | 3 |
Zn(BiO2)4 (mvc-2868) | 0.5568 | 0.151 | 3 |
Na4Mn9O18 (mp-1094147) | 0.4564 | 0.009 | 3 |
Li4(CoO2)9 (mp-851074) | 0.3729 | 0.120 | 3 |
Li4Ti3Mn6O18 (mp-769513) | 0.3251 | 0.064 | 4 |
Li4TiMn8O18 (mp-769509) | 0.2921 | 0.070 | 4 |
Li4Ti2Mn7O18 (mp-769508) | 0.2858 | 0.072 | 4 |
Li4Ti4V5O18 (mp-769487) | 0.2701 | 0.080 | 4 |
Li4Ti4Cr5O18 (mp-861696) | 0.3005 | 0.103 | 4 |
In6Se7 (mp-567596) | 0.7063 | 0.042 | 2 |
In6S7 (mp-555853) | 0.6373 | 0.008 | 2 |
Li4Ti4Mn4CoO18 (mp-775678) | 0.2882 | 0.080 | 5 |
Li4Ti3Mn4(CoO9)2 (mp-775615) | 0.1934 | 0.077 | 5 |
Li4Ti4Mn4CrO18 (mp-769455) | 0.2898 | 0.081 | 5 |
Li4Ti4Mn(Co2O9)2 (mp-769441) | 0.3008 | 0.099 | 5 |
Li4Ti3V2Cr4O18 (mp-776745) | 0.3127 | 0.092 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv Co O |
Final Energy/Atom-6.5759 eV |
Corrected Energy-455.4791 eV
-455.4791 eV = -407.7087 eV (uncorrected energy) - 25.2824 eV (MP Anion Correction) - 22.4880 eV (MP Advanced Correction)
|