Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.417 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.072 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCrO2 + Li3VO4 + LiVO2 + V2O3 |
Band Gap0.904 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 1> | 316.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 238.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 122.8 |
AlN (mp-661) | <1 1 0> | <1 -1 0> | 273.3 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 214.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 357.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 -1> | 257.6 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 204.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 268.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 238.5 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 216.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 245.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 325.2 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 334.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 328.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 328.0 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 204.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 257.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 298.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 328.0 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 328.0 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 -1> | 286.3 |
InAs (mp-20305) | <1 1 0> | <0 1 -1> | 269.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 268.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 268.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 268.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 238.5 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 253.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 238.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 208.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 328.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 149.1 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 204.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 208.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 268.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 238.5 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 271.0 |
TePb (mp-19717) | <1 0 0> | <1 1 1> | 204.3 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 204.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 298.2 |
Te2Mo (mp-602) | <1 1 1> | <0 1 1> | 278.4 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 271.0 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 122.8 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 216.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 328.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 149.1 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 268.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 -1 0> | 273.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 245.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 238.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li4(FeO2)5 (mp-762455) | 0.1998 | 0.198 | 3 |
Li7(NiO2)9 (mp-762007) | 0.2242 | 0.018 | 3 |
Li3(CoO2)4 (mp-764781) | 0.2412 | 0.129 | 3 |
Li6Ti2O7 (mp-770456) | 0.2374 | 0.019 | 3 |
Li8V11O22 (mp-768084) | 0.1399 | 0.043 | 3 |
Li3Cr3CoO8 (mp-769711) | 0.1624 | 0.442 | 4 |
Li3Fe3CoO8 (mp-763428) | 0.1291 | 0.283 | 4 |
Li3CrFe3O8 (mp-769977) | 0.1731 | 1.242 | 4 |
Li3VCr3O8 (mp-769583) | 0.1233 | 0.039 | 4 |
Li3Cr3FeO8 (mp-770226) | 0.1457 | 0.808 | 4 |
Ni6O7 (mp-767815) | 0.2084 | 0.047 | 2 |
Fe8O9 (mp-763787) | 0.2674 | 0.063 | 2 |
Fe9O10 (mp-763441) | 0.2263 | 0.040 | 2 |
Fe7O8 (mp-715333) | 0.2150 | 0.064 | 2 |
Fe8O9 (mp-705588) | 0.1985 | 0.050 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.3883 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Cr_pv O |
Final Energy/Atom-7.0534 eV |
Corrected Energy-236.9552 eV
-236.9552 eV = -211.6005 eV (uncorrected energy) - 14.1180 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)