material

Fe(CO3)2

ID:

mp-752929


Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
AFM
Formation Energy / Atom
-1.648 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.068 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.62 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CO2 + Fe2O3 + O2
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3 [148]
Hall
-R 3
Point Group
3
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
ZnO (mp-2133) <0 0 1> <0 0 1> 0.000 177.9
AlN (mp-661) <0 0 1> <0 0 1> 0.000 59.3
CdS (mp-672) <1 0 0> <1 0 0> 0.002 231.5
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.002 79.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.002 79.1
Ni (mp-23) <1 1 1> <0 0 1> 0.004 257.0
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.010 308.7
ZrO2 (mp-2858) <1 0 0> <1 0 0> 0.015 308.7
Ag (mp-124) <1 0 0> <0 0 1> 0.019 138.4
Al (mp-134) <1 1 1> <0 0 1> 0.021 257.0
GaTe (mp-542812) <1 0 0> <0 0 1> 0.022 177.9
GaSe (mp-1943) <0 0 1> <0 0 1> 0.023 237.2
LiF (mp-1138) <1 1 1> <0 0 1> 0.025 257.0
Au (mp-81) <1 0 0> <0 0 1> 0.026 138.4
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.026 19.8
LiGaO2 (mp-5854) <1 0 1> <1 1 0> 0.026 133.7
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.026 308.7
BN (mp-984) <0 0 1> <0 0 1> 0.029 138.4
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.030 154.3
LaF3 (mp-905) <0 0 1> <0 0 1> 0.038 138.4
WS2 (mp-224) <1 0 0> <1 0 0> 0.040 231.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.040 257.0
C (mp-48) <0 0 1> <0 0 1> 0.045 257.0
MgAl2O4 (mp-3536) <1 0 0> <1 1 0> 0.063 133.7
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.065 308.7
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.070 257.0
GaN (mp-804) <1 0 0> <1 0 0> 0.072 154.3
Cu (mp-30) <1 1 0> <0 0 1> 0.073 296.5
GaN (mp-804) <0 0 1> <0 0 1> 0.075 79.1
Au (mp-81) <1 1 0> <0 0 1> 0.075 98.8
LaF3 (mp-905) <1 1 0> <0 0 1> 0.075 276.7
SiC (mp-7631) <0 0 1> <0 0 1> 0.084 59.3
LiGaO2 (mp-5854) <1 0 0> <1 0 0> 0.085 308.7
Ag (mp-124) <1 1 0> <0 0 1> 0.088 98.8
SiC (mp-11714) <0 0 1> <0 0 1> 0.089 59.3
C (mp-48) <1 1 1> <0 0 1> 0.090 237.2
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.090 158.1
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.095 276.7
WSe2 (mp-1821) <1 1 1> <0 0 1> 0.106 257.0
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.109 177.9
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.109 177.9
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.112 296.5
TiO2 (mp-390) <1 1 0> <1 0 0> 0.116 154.3
LiF (mp-1138) <1 1 0> <1 0 0> 0.117 231.5
GaTe (mp-542812) <0 0 1> <0 0 1> 0.118 296.5
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.121 158.1
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.122 154.3
Ni (mp-23) <1 0 0> <0 0 1> 0.127 217.4
Ge (mp-32) <1 1 0> <1 0 0> 0.129 231.5
InSb (mp-20012) <1 0 0> <1 0 0> 0.130 308.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
V(CO3)2 (mp-762227) 0.2058 0.078 3
V(CO3)2 (mp-763352) 0.2887 0.075 3
Mn(CO3)2 (mp-768036) 0.1208 0.068 3
Co(NO3)2 (mp-542071) 0.3857 0.000 3
Pt(NO3)2 (mp-1079006) 0.2621 0.259 3
LiV2(CO3)4 (mp-763717) 0.3256 0.049 4
SrSn(BO3)2 (mp-8000) 0.5720 0.000 4
LiV2(CO3)4 (mp-763601) 0.6432 0.051 4
Li2V3(CO3)6 (mp-763569) 0.4527 0.051 4
Li2Cr3(CO3)6 (mp-763398) 0.3627 0.050 4
KAlH2CO5 (mp-644285) 0.6500 0.000 5
SiH12C2(NF)6 (mp-697253) 0.7370 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Fe_pv C O
Final Energy/Atom
-7.1665 eV
Corrected Energy
-285.7796 eV
-285.7796 eV = -257.9926 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)