Final Magnetic Moment0.248 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.236 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.043 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Fe2(PO4)3 + LiFe(CO3)2 + CO2 + Li3PO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 306.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 265.7 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 298.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 166.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 332.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 298.9 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 171.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 33.2 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 207.5 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 197.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 217.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 365.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 166.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 365.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 329.6 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 122.5 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 232.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 122.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 265.7 |
AlN (mp-661) | <1 1 1> | <1 1 -1> | 223.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 329.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 342.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 271.4 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 342.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 332.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 298.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 272.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 245.1 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 213.8 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 223.7 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 236.5 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 265.7 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 245.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 66.4 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 256.5 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 99.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 265.7 |
LiF (mp-1138) | <1 1 0> | <1 1 -1> | 298.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 265.7 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 61.3 |
TePb (mp-19717) | <1 1 1> | <1 0 -1> | 306.3 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 256.5 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 271.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 265.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 265.7 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 99.6 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 183.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 65.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 166.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 99.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li9V12Te7O48 (mp-849282) | 0.6434 | 0.061 | 4 |
Li3V(BO2)5 (mp-770344) | 0.6368 | 0.061 | 4 |
Na3Ca(BO2)5 (mp-614628) | 0.6548 | 0.001 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.6360 | 0.062 | 4 |
ZnAg3P3O13 (mvc-10277) | 0.6474 | 0.086 | 4 |
Li3Fe2P2(CO7)2 (mp-770177) | 0.1101 | 0.041 | 5 |
Li3Fe2P2(CO7)2 (mp-770153) | 0.1614 | 0.043 | 5 |
Li3Fe2P2(CO7)2 (mp-770052) | 0.1557 | 0.044 | 5 |
Li3Fe2P2(CO7)2 (mp-770292) | 0.1896 | 0.042 | 5 |
Li3Fe2P2(CO7)2 (mp-770207) | 0.1537 | 0.041 | 5 |
Li12VCr3P4(CO7)4 (mp-767735) | 0.7049 | 0.078 | 6 |
KLiMnPCO7 (mp-764256) | 0.6292 | 0.000 | 6 |
Li6MnNiP2(CO7)2 (mp-767293) | 0.7078 | 0.050 | 6 |
Li6VCrP2(CO7)2 (mp-767288) | 0.7129 | 0.078 | 6 |
NaLiMnPCO7 (mp-763833) | 0.6580 | 0.001 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P C O |
Final Energy/Atom-6.8320 eV |
Corrected Energy-172.4332 eV