Final Magnetic Moment0.482 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.810 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.247 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2CrO4 + Cr2NiO4 + V2Ni3O8 + Li3VO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 288.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 110.9 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 244.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 166.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 238.9 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 288.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 298.6 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 288.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 332.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 179.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 288.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 238.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 166.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 163.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 119.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 277.2 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 244.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 119.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 59.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 277.2 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 288.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 113.2 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 192.3 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 163.3 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 298.6 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 119.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 179.2 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 179.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 55.4 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 332.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 179.2 |
GdScO3 (mp-5690) | <0 1 1> | <0 1 1> | 113.2 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 238.9 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 238.9 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 332.6 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 332.6 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 238.9 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 238.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 288.4 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 119.5 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 96.1 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 179.2 |
Ga2O3 (mp-886) | <0 1 0> | <1 0 0> | 277.2 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 55.4 |
Ga2O3 (mp-886) | <1 0 1> | <1 0 0> | 221.7 |
Au (mp-81) | <1 1 0> | <0 0 1> | 119.5 |
Au (mp-81) | <1 1 1> | <0 0 1> | 59.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 221.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 55.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 238.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(FeO2)2 (mp-771571) | 0.3685 | 0.074 | 3 |
Li7W5O16 (mp-771579) | 0.3141 | 0.058 | 3 |
Ca(CoO2)2 (mvc-5503) | 0.3846 | 0.151 | 3 |
Ca(WO2)2 (mvc-10486) | 0.3862 | 0.384 | 3 |
Fe2GeS4 (mp-21086) | 0.3873 | 0.155 | 3 |
Li7Mn3(WO8)2 (mp-771587) | 0.1887 | 0.077 | 4 |
Li4Ti5Ni3O16 (mp-771465) | 0.1890 | 0.041 | 4 |
Li4Ti5Fe3O16 (mp-777591) | 0.1906 | 0.035 | 4 |
Li4Mn3Nb5O16 (mp-772467) | 0.2088 | 0.093 | 4 |
Li4V5Co3O16 (mp-776751) | 0.1425 | 0.108 | 4 |
Si3N4 (mp-641539) | 0.4681 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.4373 | 0.208 | 2 |
Mn3N4 (mp-1080204) | 0.4800 | 0.073 | 2 |
Cr3N4 (mp-1014358) | 0.4961 | 0.227 | 2 |
Re3N4 (mp-1080201) | 0.5308 | 0.110 | 2 |
Li4Ti3Nb2Ni3O16 (mp-771559) | 0.1783 | 0.015 | 5 |
Li4Ti2Nb3Fe3O16 (mp-762474) | 0.1555 | 0.073 | 5 |
Li4Nb2V3Ni3O16 (mp-777087) | 0.1625 | 0.024 | 5 |
Li4Ti3Mn3Nb2O16 (mp-776061) | 0.1446 | 0.042 | 5 |
Li4V2Co3Ni3O16 (mp-763125) | 0.1434 | 0.081 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6804 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764708) | 0.6889 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6859 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.6922 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6850 | 0.661 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVCr: 3.7 eV Ni: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Cr_pv Ni_pv O |
Final Energy/Atom-6.2432 eV |
Corrected Energy-201.9412 eV
-201.9412 eV = -174.8096 eV (uncorrected energy) - 15.8950 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)