material

LiFe2O3

ID:

mp-756381


Material Details

Final Magnetic Moment
0.059 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FiM
Formation Energy / Atom
-1.863 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.094 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.68 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
LiFeO2 + FeO
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaSe (mp-1943) <0 0 1> <0 0 1> 0.000 151.4
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.002 199.2
Ni (mp-23) <1 1 0> <1 1 0> 0.002 156.5
InAs (mp-20305) <1 1 1> <0 0 1> 0.005 199.2
Mg (mp-153) <1 0 0> <1 1 0> 0.006 117.4
TeO2 (mp-2125) <0 0 1> <1 0 0> 0.007 226.0
InP (mp-20351) <1 1 1> <0 0 1> 0.011 247.0
GaN (mp-804) <1 1 0> <1 1 0> 0.014 117.4
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.020 39.1
NaCl (mp-22862) <1 1 1> <0 0 1> 0.021 55.8
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.024 158.2
CdSe (mp-2691) <1 1 1> <0 0 1> 0.028 199.2
GaN (mp-804) <1 0 0> <1 1 0> 0.031 117.4
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.032 234.8
LiNbO3 (mp-3731) <1 0 0> <0 0 1> 0.035 223.1
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.037 143.4
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.041 223.1
Mg (mp-153) <1 0 1> <1 0 0> 0.042 113.0
BN (mp-984) <0 0 1> <0 0 1> 0.043 71.7
GaSb (mp-1156) <1 1 1> <0 0 1> 0.046 199.2
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.047 151.4
C (mp-48) <1 1 1> <0 0 1> 0.049 167.3
Fe3O4 (mp-19306) <1 1 1> <0 0 1> 0.061 127.5
LiTaO3 (mp-3666) <1 0 1> <0 0 1> 0.062 231.0
YAlO3 (mp-3792) <1 1 1> <1 0 0> 0.065 248.6
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.065 199.2
PbS (mp-21276) <1 1 1> <0 0 1> 0.067 247.0
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.069 199.2
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.073 23.9
BN (mp-984) <1 0 1> <1 0 0> 0.073 180.8
PbSe (mp-2201) <1 1 1> <0 0 1> 0.075 199.2
MgO (mp-1265) <1 0 0> <1 0 0> 0.077 90.4
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.078 113.0
KCl (mp-23193) <1 1 1> <0 0 1> 0.079 71.7
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.079 47.8
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.080 156.5
PbS (mp-21276) <1 0 0> <1 0 0> 0.086 180.8
Ga2O3 (mp-886) <1 1 -1> <1 0 1> 0.087 239.6
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.094 310.7
GaN (mp-804) <1 0 1> <1 0 0> 0.094 113.0
ZrO2 (mp-2858) <1 0 1> <0 0 1> 0.095 127.5
KCl (mp-23193) <1 1 0> <1 1 0> 0.096 117.4
LiNbO3 (mp-3731) <1 0 1> <0 0 1> 0.100 231.0
CdS (mp-672) <1 0 0> <0 0 1> 0.102 199.2
Te2W (mp-22693) <1 0 0> <0 0 1> 0.105 294.8
GaTe (mp-542812) <0 1 0> <0 0 1> 0.106 191.2
Mg (mp-153) <1 1 0> <1 1 0> 0.107 117.4
Ni (mp-23) <1 1 1> <0 0 1> 0.112 151.4
GdScO3 (mp-5690) <0 1 1> <0 0 1> 0.114 326.6
TbScO3 (mp-31119) <0 1 1> <0 0 1> 0.115 326.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
InCuSe2 (mp-676764) 0.1708 0.204 3
Li2Ni5O7 (mp-767264) 0.1722 0.273 3
Li2BiO3 (mp-769002) 0.1769 0.033 3
CaMnO2 (mp-1003322) 0.1756 0.017 3
LiMnO2 (mp-25539) 0.1693 0.100 3
Li2VFeO4 (mp-770982) 0.1285 0.044 4
Li3Cr2CuO6 (mp-997512) 0.1318 0.250 4
Li2VCrO4 (mp-768055) 0.1296 0.006 4
Li4V3CrO8 (mp-768054) 0.1316 0.027 4
Li3NiOF3 (mp-765893) 0.1234 0.086 4
Bi2Te3 (mp-568390) 0.1943 0.248 2
AgBr (mp-570301) 0.2234 0.042 2
In2Se3 (mp-1068548) 0.2370 0.530 2
RbN (mp-1066707) 0.2343 1.513 2
In2Se3 (mp-20830) 0.1927 0.530 2
Na6MnNi3(SbO6)2 (mp-1094109) 0.6433 0.139 5
Hg (mp-982872) 0.3238 0.020 1
Sb (mp-632286) 0.3401 0.059 1
Se (mp-7755) 0.3948 0.181 1
Te (mp-10654) 0.3547 0.047 1
Te (mp-105) 0.2666 0.047 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Fe: 5.3 eV
Pseudopotentials
VASP PAW: Li_sv Fe_pv O
Final Energy/Atom
-6.2163 eV
Corrected Energy
-43.8711 eV
Uncorrected energy = -37.2981 eV Composition-based energy adjustment (-0.687 eV/atom x 3.0 atoms) = -2.0610 eV Composition-based energy adjustment (-2.256 eV/atom x 2.0 atoms) = -4.5120 eV Corrected energy = -43.8711 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)