Final Magnetic Moment16.999 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.738 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.113 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.07 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoO2 + LiCrO2 + CoO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 343.6 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 291.9 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 194.6 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 171.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 308.5 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 294.6 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 153.8 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 294.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 97.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 137.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 308.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 34.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 48.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 171.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 68.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 240.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 171.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 274.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 34.3 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 48.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 59.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 245.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 205.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 274.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 34.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 48.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 196.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 171.4 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 245.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 171.4 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 230.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 59.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 118.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 177.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 146.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 171.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 167.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 308.5 |
BN (mp-984) | <1 0 0> | <1 0 0> | 308.5 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 243.3 |
BN (mp-984) | <1 1 0> | <1 1 0> | 239.5 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 243.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 230.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 171.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 343.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 146.0 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 -1> | 243.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 118.4 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 291.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 274.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5Fe7O12 (mp-771531) | 0.1668 | 0.025 | 3 |
LiCoO2 (mp-853240) | 0.1681 | 0.075 | 3 |
Li5Fe11O16 (mp-762692) | 0.1557 | 0.043 | 3 |
Li5Fe11O16 (mp-768075) | 0.1392 | 0.020 | 3 |
Li3Fe5O8 (mp-586092) | 0.1676 | 0.484 | 3 |
Li5Fe5(NiO6)2 (mp-771555) | 0.1252 | 0.027 | 4 |
Li3Cu(NiO2)4 (mp-772355) | 0.1292 | 0.032 | 4 |
Li4TiFe3O8 (mp-769962) | 0.1252 | 0.314 | 4 |
Li2CoNiO4 (mp-765786) | 0.1076 | 0.017 | 4 |
Li3Co4NiO8 (mp-771085) | 0.0951 | 0.043 | 4 |
LiTe3 (mp-27466) | 0.2188 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.3338 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.2957 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.3128 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.3005 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.4849 | 0.139 | 5 |
Hg (mp-982872) | 0.4859 | 0.020 | 1 |
Sb (mp-632286) | 0.4384 | 0.059 | 1 |
Te (mp-570459) | 0.5003 | 0.044 | 1 |
Te (mp-10654) | 0.5383 | 0.047 | 1 |
Te (mp-105) | 0.4177 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Co O |
Final Energy/Atom-6.0044 eV |
Corrected Energy-110.1177 eV
Uncorrected energy = -96.0707 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-1.999 eV/atom x 1.0 atoms) = -1.9990 eV
Composition-based energy adjustment (-1.638 eV/atom x 4.0 atoms) = -6.5520 eV
Corrected energy = -110.1177 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)