Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.518 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiMnBO3 |
Band Gap2.847 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 286.3 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 -1> | 243.5 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 0> | 260.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 260.8 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 89.6 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 149.3 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 167.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 190.4 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 83.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 309.4 |
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 243.5 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 289.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 231.8 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 222.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 285.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 119.0 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 286.3 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 119.4 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 243.5 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 133.1 |
GaN (mp-804) | <1 0 1> | <0 1 -1> | 130.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 142.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 266.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 173.9 |
SiO2 (mp-6930) | <1 1 0> | <1 -1 1> | 253.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 237.9 |
KCl (mp-23193) | <1 1 1> | <1 0 0> | 286.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 119.0 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 285.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 89.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 328.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 209.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 -1 1> | 126.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 212.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 0> | 265.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 0> | 324.4 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 159.0 |
InAs (mp-20305) | <1 1 1> | <1 1 -1> | 340.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 119.0 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 289.8 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 222.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 222.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 261.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 159.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 328.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 173.9 |
CdS (mp-672) | <1 0 0> | <0 1 -1> | 228.4 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 318.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 254.4 |
CdS (mp-672) | <1 0 1> | <1 -1 1> | 126.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2MnF4 (mp-764846) | 0.6711 | 0.062 | 3 |
Li3BO3 (mp-27275) | 0.5720 | 0.000 | 3 |
Li6B4O9 (mp-768875) | 0.7001 | 0.063 | 3 |
Na3CoO3 (mp-777919) | 0.4122 | 0.018 | 3 |
Li6B4O9 (mp-1020024) | 0.7086 | 0.000 | 3 |
LiMnBO3 (mp-849500) | 0.3424 | 0.000 | 4 |
LiCoBO3 (mp-766795) | 0.3410 | 0.139 | 4 |
LiCrBO3 (mp-770242) | 0.2987 | 0.050 | 4 |
LiFeBO3 (mp-777711) | 0.3213 | 0.000 | 4 |
LiFeBO3 (mp-783910) | 0.3251 | 0.000 | 4 |
Li8Mn7Fe(BO3)8 (mp-850226) | 0.0471 | 0.003 | 5 |
Li8Mn7Fe(BO3)8 (mp-779867) | 0.0528 | 0.003 | 5 |
Li8Mn7Fe(BO3)8 (mp-779267) | 0.0529 | 0.003 | 5 |
Li4Mn3Fe(BO3)4 (mp-774076) | 0.0500 | 0.014 | 5 |
Li8Mn7Fe(BO3)8 (mp-778353) | 0.0583 | 0.003 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv B O |
Final Energy/Atom-7.3191 eV |
Corrected Energy-190.8091 eV
-190.8091 eV = -175.6582 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)