Final Magnetic Moment19.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.740 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.060 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.49 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Mn3NiO8 + Li(NiO2)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 107.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 232.1 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 221.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 248.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 160.9 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 160.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 160.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 116.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 323.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 174.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 290.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 160.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 232.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 323.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 232.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 161.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 58.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 269.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 116.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 58.0 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 269.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 174.1 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 215.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 58.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 174.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 174.1 |
BN (mp-984) | <1 1 0> | <0 0 1> | 232.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 116.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 161.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 116.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 58.0 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 174.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 283.5 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 269.3 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 160.9 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 215.4 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 232.1 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 215.4 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 232.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 58.0 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 174.1 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 174.1 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 53.9 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 290.1 |
Au (mp-81) | <1 0 0> | <0 0 1> | 174.1 |
Au (mp-81) | <1 1 0> | <1 0 0> | 215.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 58.0 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 116.0 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 269.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li(FeO2)2 (mp-771571) | 0.1288 | 0.666 | 3 |
LiCr2O4 (mp-771523) | 0.1939 | 0.088 | 3 |
Ca(MoO2)2 (mvc-6227) | 0.2269 | 0.228 | 3 |
Li(NiO2)2 (mp-771429) | 0.2282 | 0.063 | 3 |
LiTi2O4 (mp-776170) | 0.2104 | 0.042 | 3 |
Li2V3FeO8 (mp-775524) | 0.1312 | 0.238 | 4 |
Li4Mn5Cr3O16 (mp-772402) | 0.1082 | 0.054 | 4 |
Li4Mn5Cu3O16 (mp-761365) | 0.1284 | 0.058 | 4 |
Li4Fe5Cu3O16 (mp-771929) | 0.1014 | 0.069 | 4 |
Li4Fe5Ni3O16 (mp-771734) | 0.1341 | 0.122 | 4 |
Si3N4 (mp-641539) | 0.3718 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.3806 | 0.208 | 2 |
Mn3N4 (mp-1080204) | 0.3327 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.3065 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.3650 | 0.060 | 2 |
Li4Mn2Fe3Co3O16 (mp-761441) | 0.1268 | 0.078 | 5 |
Li4Ti2Fe3Co3O16 (mp-762763) | 0.1205 | 0.087 | 5 |
Li4Mn3Cr3(FeO8)2 (mp-761449) | 0.1149 | 0.570 | 5 |
Li4Mn3Co2Ni3O16 (mp-868013) | 0.0857 | 0.078 | 5 |
Li4Ti3Cr3(FeO8)2 (mp-776639) | 0.1166 | 0.597 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.7098 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6984 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7028 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7050 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7068 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Ni_pv O |
Final Energy/Atom-6.1618 eV |
Corrected Energy-198.6630 eV
-198.6630 eV = -172.5301 eV (uncorrected energy) - 14.8963 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|