Final Magnetic Moment2.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.355 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.038 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi4Ni3Sn5O16 + Li(NiO2)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 207.0 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 111.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 126.2 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 252.4 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 315.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 207.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 167.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 236.6 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 207.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 118.3 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 252.4 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 252.4 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 334.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 325.3 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 289.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 207.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 222.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 236.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 55.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 207.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 167.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 236.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 147.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 118.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.6 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 207.0 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 354.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 147.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 118.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.6 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 266.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 278.7 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 193.1 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 193.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 207.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 266.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 88.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 118.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 29.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 118.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 88.7 |
GaSe (mp-1943) | <1 0 1> | <1 1 1> | 201.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 88.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 325.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 266.2 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 207.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 207.0 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 201.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 147.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMn2O4 (mp-771583) | 0.1431 | 0.023 | 3 |
Li(FeO2)2 (mp-771571) | 0.1588 | 0.102 | 3 |
LiCr2O4 (mp-771523) | 0.2171 | 0.034 | 3 |
Li(NiO2)2 (mp-771429) | 0.0894 | 0.060 | 3 |
LiTi2O4 (mp-776170) | 0.2108 | 0.040 | 3 |
Li2Co3SnO8 (mp-772420) | 0.1211 | 0.027 | 4 |
Li2Mn3NiO8 (mp-772391) | 0.1175 | 0.052 | 4 |
Li2CrCo3O8 (mp-766712) | 0.1369 | 0.054 | 4 |
Li2Mn3CoO8 (mp-769908) | 0.1277 | 0.035 | 4 |
Li2Cr3SnO8 (mp-769749) | 0.0796 | 0.011 | 4 |
Si3N4 (mp-641539) | 0.3537 | 0.287 | 2 |
Ge3N4 (mp-641541) | 0.3555 | 0.207 | 2 |
In3S4 (mp-556597) | 0.3891 | 0.048 | 2 |
Cr3N4 (mp-1014358) | 0.3323 | 0.099 | 2 |
Fe3O4 (mp-650112) | 0.3811 | 0.041 | 2 |
Li4Mn3Cr3(SnO8)2 (mp-776805) | 0.1409 | 0.008 | 5 |
Li4Mn3Fe2Co3O16 (mp-775386) | 0.1202 | 0.025 | 5 |
Li4Mn3Cr3(FeO8)2 (mp-761449) | 0.1268 | 0.041 | 5 |
Li4Ti3Mn3(NiO8)2 (mp-770507) | 0.1237 | 0.062 | 5 |
Li4Cr3Co3(SnO8)2 (mp-778219) | 0.1485 | 0.035 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7151 | 0.030 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.7158 | 0.015 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.7225 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.7159 | 0.062 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.7211 | 0.012 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv Sn_d O |
Final Energy/Atom-5.1083 eV |
Corrected Energy-167.2523 eV
-167.2523 eV = -143.0317 eV (uncorrected energy) - 12.9840 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)