Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.869 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCrO2 + MnO2 |
Band Gap1.337 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 103.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 193.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 329.3 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 286.3 |
AlN (mp-661) | <1 1 0> | <1 1 -1> | 248.1 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 129.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 237.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 197.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 290.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 -1> | 248.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 286.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 263.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 95.4 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 207.3 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 259.1 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 207.3 |
MoS2 (mp-1434) | <1 0 0> | <1 0 -1> | 206.1 |
LiGaO2 (mp-5854) | <1 1 1> | <1 1 0> | 286.3 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 286.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 329.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 -1> | 103.1 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 263.4 |
C (mp-66) | <1 0 0> | <0 1 0> | 207.3 |
C (mp-66) | <1 1 0> | <1 1 0> | 286.3 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 329.3 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 237.8 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 290.3 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 197.6 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 263.4 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 207.3 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 1> | 129.6 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 329.3 |
Si (mp-149) | <1 1 0> | <1 0 1> | 129.6 |
Au (mp-81) | <1 0 0> | <1 0 1> | 259.1 |
Au (mp-81) | <1 1 0> | <0 1 0> | 276.4 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 131.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 329.3 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 237.8 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 197.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 329.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 206.1 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 193.6 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 329.3 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 276.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 329.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 290.3 |
MoS2 (mp-1434) | <0 0 1> | <1 1 -1> | 124.1 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 -1> | 248.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 193.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 290.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCrO4 (mp-772296) | 0.1137 | 0.017 | 3 |
MgCrO4 (mp-540704) | 0.1036 | 0.902 | 3 |
VInO4 (mp-541501) | 0.1865 | 0.020 | 3 |
MnMoO4 (mp-19081) | 0.2301 | 0.000 | 3 |
CrCdO4 (mp-19630) | 0.2306 | 0.013 | 3 |
Li2Fe2(PO4)3 (mp-776769) | 0.3620 | 0.030 | 4 |
V5Sb(PO4)6 (mp-770673) | 0.3920 | 0.230 | 4 |
Li2Cr2(PO4)3 (mp-777909) | 0.3993 | 0.097 | 4 |
LiZr2(PO4)3 (mp-773068) | 0.3806 | 0.012 | 4 |
LiNb2(PO4)3 (mp-26533) | 0.3941 | 0.068 | 4 |
VO2 (mvc-6918) | 0.7116 | 0.095 | 2 |
MoO2 (mvc-6944) | 0.6395 | 0.387 | 2 |
Fe3Co2Te(PO4)6 (mp-997541) | 0.4048 | 0.418 | 5 |
Ti3CuNi2(PO4)6 (mp-776876) | 0.4064 | 0.034 | 5 |
TiZnMo(PO4)3 (mvc-9207) | 0.4064 | 0.010 | 5 |
MgTiP3WO12 (mvc-9222) | 0.4066 | 0.051 | 5 |
TiZnP3WO12 (mvc-9230) | 0.4033 | 0.063 | 5 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.5207 | 0.080 | 6 |
NaLi3Ti2Fe2(PO4)6 (mp-850140) | 0.4725 | 0.114 | 6 |
NaLi3Ti2Cr2(PO4)6 (mp-777190) | 0.5305 | 0.028 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.4821 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4806 | 0.015 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Mn_pv Cr_pv O |
Final Energy/Atom-7.2189 eV |
Corrected Energy-199.2654 eV
-199.2654 eV = -173.2534 eV (uncorrected energy) - 14.7754 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)