Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.782 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.119 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.38 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr2O3 + TiO2 + Cr |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 -1> | 306.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 355.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 355.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 213.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 165.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 165.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 142.1 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 307.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 165.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 213.1 |
AlN (mp-661) | <1 1 1> | <1 1 -1> | 258.7 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 284.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 236.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 260.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 307.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 118.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 222.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 71.0 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 153.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 331.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 284.1 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 222.9 |
SiO2 (mp-6930) | <1 0 1> | <1 -1 1> | 311.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 71.0 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 263.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 165.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 355.2 |
CdS (mp-672) | <1 0 0> | <1 -1 0> | 223.3 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 229.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 284.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 213.1 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 222.1 |
Te2W (mp-22693) | <0 1 0> | <0 1 0> | 222.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 71.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 213.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 213.1 |
Te2Mo (mp-602) | <1 0 0> | <1 -1 -1> | 156.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 284.1 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 296.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 94.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 71.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 165.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 71.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 213.1 |
BN (mp-984) | <1 1 1> | <0 1 1> | 236.4 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 74.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 1 0> | 128.3 |
LiNbO3 (mp-3731) | <1 1 1> | <1 1 -1> | 129.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 23.7 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 -1> | 76.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMn2F5 (mp-764317) | 0.4360 | 0.046 | 3 |
MgCoO3 (mp-776512) | 0.4298 | 0.141 | 3 |
Li10Co4O9 (mp-773128) | 0.3762 | 0.370 | 3 |
NaMn2O4 (mp-1003736) | 0.3747 | 0.103 | 3 |
CaMn4O8 (mp-1003320) | 0.4194 | 0.059 | 3 |
Mg2Ta2MnO8 (mvc-2649) | 0.3062 | 0.003 | 4 |
Mg2Nb2CoO8 (mvc-3391) | 0.2764 | 0.018 | 4 |
Mg2MnNb2O8 (mvc-402) | 0.2876 | 0.220 | 4 |
Mg2Nb2NiO8 (mvc-418) | 0.2895 | 0.071 | 4 |
Mg2Nb2FeO8 (mvc-13319) | 0.2988 | 0.002 | 4 |
V5O9 (mp-714932) | 0.6023 | 0.017 | 2 |
Ti3O5 (mp-556754) | 0.6006 | 0.013 | 2 |
Ti4O7 (mp-12205) | 0.5961 | 0.005 | 2 |
V5O9 (mp-558587) | 0.5828 | 0.008 | 2 |
Ti4O7 (mp-558097) | 0.5988 | 0.005 | 2 |
Li4FeTe(WO6)2 (mp-771716) | 0.5716 | 0.163 | 5 |
Li4MnNb2WO12 (mp-771475) | 0.5664 | 0.046 | 5 |
Li4MnSb(WO6)2 (mp-779994) | 0.5926 | 0.041 | 5 |
Li4CrTe(WO6)2 (mp-777147) | 0.5587 | 0.075 | 5 |
Li4VFe(WO6)2 (mp-761519) | 0.5421 | 0.070 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Ti_pv Cr_pv O |
Final Energy/Atom-8.4364 eV |
Corrected Energy-277.8107 eV
-277.8107 eV = -253.0915 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction) - 12.0780 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)