Final Magnetic Moment2.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.588 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBa4Mn3O10 + BaO |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 224.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 215.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 1> | 224.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 229.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 246.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 197.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 295.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 279.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 147.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 32.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 228.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 82.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 82.1 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 168.6 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 262.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 213.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 344.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 295.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 279.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 82.1 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 224.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 311.1 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 152.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 131.3 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 228.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 164.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 65.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 147.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 32.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 228.1 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 16.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 112.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 0> | 228.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 328.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 16.4 |
Al (mp-134) | <1 1 0> | <1 0 1> | 112.4 |
Al (mp-134) | <1 1 1> | <1 1 0> | 228.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 328.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 262.7 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 224.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 213.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 16.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 114.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 147.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 295.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 268.8 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 268.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 311.9 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 131.3 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 279.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cs2MnCl4 (mp-1025252) | 0.0321 | 0.014 | 3 |
Rb2ZnF4 (mp-1025286) | 0.0792 | 0.000 | 3 |
Rb2CuCl4 (mp-974690) | 0.0700 | 0.021 | 3 |
Rb4I2O (mp-760417) | 0.0763 | 0.000 | 3 |
Cs2CrCl4 (mp-28497) | 0.0840 | 0.035 | 3 |
Pr2AlNO3 (mp-1025277) | 0.6098 | 0.071 | 4 |
Ce2AlNO3 (mp-1025275) | 0.4857 | 0.101 | 4 |
Eu2AlNO3 (mp-1025206) | 0.4347 | 0.117 | 4 |
Rb2Cr(BrCl)2 (mp-1025321) | 0.1351 | 0.010 | 4 |
Nd2AlNO3 (mp-546679) | 0.6359 | 0.077 | 4 |
SrLiLa3MnO8 (mp-767057) | 0.6477 | 0.019 | 5 |
SrLiLa3MnO8 (mp-779988) | 0.5235 | 0.025 | 5 |
SrLiLa3FeO8 (mp-767455) | 0.7447 | 0.010 | 5 |
SrLi4La15(CoO8)4 (mp-767969) | 0.7204 | 0.024 | 5 |
Sr5La5Cu(NiO5)4 (mp-690554) | 0.4976 | 0.012 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Ba_sv Mn_pv O |
Final Energy/Atom-6.6316 eV |
Corrected Energy-50.9112 eV
-50.9112 eV = -46.4212 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction) - 1.6809 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)