Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.883 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.038 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.78 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCrO2 + Al2O3 |
Band Gap0.680 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Group2/m |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 102.1 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 193.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 238.3 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 194.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 238.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 238.3 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 242.6 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 311.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 238.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 306.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 238.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 290.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 340.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 272.3 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 291.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 103.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 306.4 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 311.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 306.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 238.3 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 290.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 145.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 306.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 138.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 68.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 170.2 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 238.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 136.2 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 68.1 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 193.8 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 290.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 181.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 306.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 306.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 238.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 272.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 340.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 238.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 238.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 136.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 306.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 340.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 172.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 170.2 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 339.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 238.3 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 339.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 306.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 311.1 |
GaSe (mp-1943) | <1 1 0> | <0 1 1> | 242.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MgTi11O20 (mp-766100) | 0.2292 | 0.007 | 3 |
TiFe2O5 (mp-763506) | 0.2483 | 0.024 | 3 |
CrFe2O5 (mp-769957) | 0.2415 | 0.081 | 3 |
TiFe2O5 (mp-24977) | 0.2340 | 0.040 | 3 |
TiAl2O5 (mp-4930) | 0.1623 | 0.013 | 3 |
LiMn2O2F3 (mp-763878) | 0.3555 | 0.064 | 4 |
LiCo2O2F3 (mp-850987) | 0.4001 | 0.165 | 4 |
LiV2O2F3 (mp-765853) | 0.4039 | 0.069 | 4 |
LiV2O2F3 (mp-765822) | 0.3553 | 0.063 | 4 |
LiFe2O2F3 (mp-774121) | 0.3637 | 0.075 | 4 |
Ti3O5 (mp-8057) | 0.2620 | 0.005 | 2 |
Ta3N5 (mp-27488) | 0.3102 | 0.000 | 2 |
Nb3N5 (mp-754556) | 0.4093 | 0.018 | 2 |
Ti6O11 (mp-559964) | 0.5413 | 0.006 | 2 |
Ti3O5 (mp-556480) | 0.3363 | 0.007 | 2 |
Li4NbFe(WO6)2 (mp-850102) | 0.6221 | 0.022 | 5 |
Li4CrSb(TeO6)2 (mp-781050) | 0.6462 | 0.048 | 5 |
Li4MnNb(WO6)2 (mp-771868) | 0.5888 | 0.028 | 5 |
Li4FeBi(TeO6)2 (mp-776005) | 0.6242 | 0.036 | 5 |
Li4CrBi(TeO6)2 (mp-775998) | 0.6452 | 0.076 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Al Cr_pv O |
Final Energy/Atom-7.4277 eV |
Corrected Energy-259.7838 eV
-259.7838 eV = -237.6860 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 8.0520 eV (MP Advanced Correction)
|