Final Magnetic Moment1.998 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.662 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.088 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVBO3 + Li3PO4 |
Band Gap2.183 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 302.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 -1> | 121.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 227.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 32.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 291.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 162.2 |
AlN (mp-661) | <1 1 1> | <1 1 -1> | 222.4 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 235.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 259.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 324.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 291.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 121.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 227.1 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 170.9 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 66.0 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 170.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 194.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 326.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 356.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 194.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 291.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 324.4 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 121.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 227.1 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 -1> | 222.4 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 268.2 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 213.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 324.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 291.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 242.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 291.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 259.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 324.4 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 148.2 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 235.9 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 256.3 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 259.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 170.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 259.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 66.0 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 276.7 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 97.3 |
Te2W (mp-22693) | <1 0 1> | <1 0 1> | 198.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 259.5 |
YVO4 (mp-19133) | <1 0 0> | <1 0 -1> | 181.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 64.9 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 129.7 |
TePb (mp-19717) | <1 1 0> | <1 0 -1> | 60.6 |
TePb (mp-19717) | <1 1 1> | <1 0 -1> | 302.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 299.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiAgF3 (mp-752605) | 0.7034 | 0.051 | 3 |
Li9V19O48 (mp-777033) | 0.6523 | 0.102 | 3 |
Li9Cr19O48 (mp-851274) | 0.7038 | 0.074 | 3 |
MnVO4 (mp-771856) | 0.6911 | 0.078 | 3 |
CuSeO4 (mp-554040) | 0.6924 | 0.000 | 3 |
Li3MnSi2O7 (mp-780126) | 0.5891 | 0.084 | 4 |
Li3Si2BiO7 (mp-757466) | 0.5753 | 0.058 | 4 |
MgVPO5 (mvc-3281) | 0.5705 | 0.217 | 4 |
MnZnPO5 (mvc-3247) | 0.5217 | 0.029 | 4 |
Li2Mo(PO4)2 (mp-540435) | 0.6068 | 0.069 | 4 |
Li3MnBAsO7 (mp-771436) | 0.2541 | 0.091 | 5 |
Li3SiSnBO7 (mp-770756) | 0.1886 | 0.059 | 5 |
Li3CrBPO7 (mp-770034) | 0.1707 | 0.077 | 5 |
Li3FeBPO7 (mp-771744) | 0.3099 | 0.234 | 5 |
Li3MnBPO7 (mp-771732) | 0.2070 | 0.080 | 5 |
Li12CoNi3P4(CO7)4 (mp-767857) | 0.5654 | 0.036 | 6 |
Li12FeNi3P4(CO7)4 (mp-767731) | 0.5583 | 0.036 | 6 |
Li6MnNiP2(CO7)2 (mp-767293) | 0.5540 | 0.046 | 6 |
Li6CoNiP2(CO7)2 (mp-767291) | 0.5684 | 0.038 | 6 |
Li6FeNiP2(CO7)2 (mp-767289) | 0.5376 | 0.041 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv B P O |
Final Energy/Atom-6.8881 eV |
Corrected Energy-192.2856 eV
-192.2856 eV = -179.0896 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 3.3640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)