material

Y2V2O7

ID:

mp-754039


Material Details

Final Magnetic Moment
2.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FiM
Formation Energy / Atom
-3.153 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.082 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.94 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
YVO3 + YVO4
Band Gap
0.536 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/m [12]
Hall
-C 2y
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <1 0 0> <1 0 0> 0.003 50.0
Te2W (mp-22693) <0 0 1> <1 0 0> 0.008 200.1
GaP (mp-2490) <1 1 0> <0 0 1> 0.009 128.2
Te2W (mp-22693) <1 0 0> <1 0 -1> 0.011 294.6
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.012 128.2
Ga2O3 (mp-886) <1 0 -1> <0 1 0> 0.013 346.2
Ni (mp-23) <1 1 0> <1 1 0> 0.014 121.7
AlN (mp-661) <1 1 1> <1 0 0> 0.021 200.1
CdS (mp-672) <1 0 1> <1 0 -1> 0.024 294.6
BN (mp-984) <0 0 1> <1 0 0> 0.027 250.1
TiO2 (mp-390) <1 0 1> <1 0 0> 0.029 200.1
DyScO3 (mp-31120) <0 1 0> <0 1 0> 0.029 173.1
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.032 128.2
ZrO2 (mp-2858) <0 0 1> <0 1 0> 0.034 138.5
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.038 100.0
CdWO4 (mp-19387) <1 0 1> <1 0 -1> 0.039 220.9
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.041 320.6
CdSe (mp-2691) <1 0 0> <0 1 0> 0.043 346.2
Al2O3 (mp-1143) <1 0 0> <1 0 0> 0.047 250.1
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.053 250.1
LiNbO3 (mp-3731) <1 0 1> <0 1 0> 0.054 311.6
ZnTe (mp-2176) <1 0 0> <0 1 0> 0.054 346.2
GaSb (mp-1156) <1 0 0> <0 1 0> 0.054 346.2
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.055 320.6
WS2 (mp-224) <1 0 1> <0 0 1> 0.055 320.6
Al2O3 (mp-1143) <1 0 1> <1 0 1> 0.060 265.0
InAs (mp-20305) <1 0 0> <0 1 0> 0.062 346.2
Si (mp-149) <1 1 0> <0 0 1> 0.073 128.2
YAlO3 (mp-3792) <1 1 0> <0 1 0> 0.074 277.0
PbSe (mp-2201) <1 0 0> <0 1 0> 0.076 346.2
DyScO3 (mp-31120) <1 0 1> <1 0 -1> 0.078 220.9
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.080 128.2
DyScO3 (mp-31120) <0 1 1> <0 0 1> 0.084 320.6
ZnO (mp-2133) <1 1 0> <1 0 0> 0.085 150.1
Ga2O3 (mp-886) <1 0 0> <0 1 1> 0.087 72.9
TbScO3 (mp-31119) <0 1 0> <0 1 0> 0.088 173.1
ZrO2 (mp-2858) <0 1 0> <0 1 0> 0.091 138.5
GaN (mp-804) <1 0 0> <1 0 0> 0.099 50.0
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.100 256.4
NdGaO3 (mp-3196) <1 1 0> <1 1 -1> 0.101 244.1
Si (mp-149) <1 1 1> <0 0 1> 0.106 256.4
C (mp-66) <1 1 1> <0 1 1> 0.110 291.4
Mg (mp-153) <1 1 0> <1 0 0> 0.121 200.1
YAlO3 (mp-3792) <0 1 1> <1 1 0> 0.122 243.3
CaF2 (mp-2741) <1 0 0> <1 1 -1> 0.123 244.1
TbScO3 (mp-31119) <0 1 1> <0 0 1> 0.126 320.6
LiAlO2 (mp-3427) <0 0 1> <0 1 0> 0.129 138.5
CaCO3 (mp-3953) <0 0 1> <0 1 1> 0.129 291.4
NdGaO3 (mp-3196) <1 0 0> <1 0 -1> 0.135 220.9
LiF (mp-1138) <1 0 0> <1 1 1> 0.137 284.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
V2Zn2O7 (mp-634381) 0.3688 0.031 3
Dy2V2O7 (mp-783902) 0.0359 0.072 3
Ho2V2O7 (mp-769888) 0.1178 0.068 3
Mn2V2O7 (mp-19142) 0.1337 0.000 3
Ni2As2O7 (mp-25092) 0.2701 0.024 3
ZrO2 (mp-755769) 0.7329 0.052 2
NbO2 (mp-754698) 0.7453 0.107 2
TiO2 (mp-554278) 0.7412 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
V: 3.25 eV
Pseudopotentials
VASP PAW: Y_sv V_pv O
Final Energy/Atom
-8.3763 eV
Corrected Energy
-100.4192 eV
-100.4192 eV = -92.1392 eV (uncorrected energy) - 4.9160 eV (MP Anion Correction) - 3.3640 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by