Final Magnetic Moment1.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.995 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.063 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2O2 + Li2O + Li2MnO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 226.9 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 226.9 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 295.1 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 -1> | 258.2 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 226.9 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 184.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 90.8 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 256.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 90.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 -1> | 258.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 68.1 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 332.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 347.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 260.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 110.7 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 294.9 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 147.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 90.8 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 312.4 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 284.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 110.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 22.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 113.4 |
CdS (mp-672) | <0 0 1> | <1 0 -1> | 258.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 258.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 295.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 284.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 284.0 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 204.2 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 255.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 186.7 |
LiF (mp-1138) | <1 1 0> | <1 1 -1> | 255.3 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 247.8 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 272.3 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 186.7 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 258.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 156.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 45.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 181.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 68.1 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 332.0 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 208.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 272.3 |
Te2Mo (mp-602) | <1 0 1> | <0 1 1> | 320.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 272.3 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 294.9 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 68.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 68.1 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 113.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 258.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5NbO5 (mp-770649) | 0.2901 | 0.021 | 3 |
Na5BiO5 (mp-760400) | 0.2669 | 0.000 | 3 |
Li5SbO5 (mp-29364) | 0.2198 | 0.000 | 3 |
Li5BiO5 (mp-29365) | 0.2318 | 0.000 | 3 |
Li5TaO5 (mp-755013) | 0.3084 | 0.000 | 3 |
Li3Fe2OF5 (mp-773547) | 0.3823 | 0.110 | 4 |
Li5NiO3F2 (mp-764683) | 0.4151 | 0.093 | 4 |
Li3Co2OF5 (mp-849429) | 0.3628 | 0.488 | 4 |
Li3Ni2OF5 (mp-859785) | 0.3889 | 0.091 | 4 |
Li3Mn2OF5 (mp-767181) | 0.3191 | 0.099 | 4 |
Ti10O13 (mp-753593) | 0.5837 | 0.028 | 2 |
Fe13O15 (mp-767312) | 0.4867 | 0.601 | 2 |
Ti11O14 (mp-759754) | 0.5042 | 0.047 | 2 |
Fe3O4 (mp-715614) | 0.6283 | 0.468 | 2 |
Nb16N13 (mp-32913) | 0.5593 | 0.102 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O |
Final Energy/Atom-5.4729 eV |
Corrected Energy-65.3941 eV
-65.3941 eV = -60.2018 eV (uncorrected energy) - 3.5114 eV (MP Anion Correction) - 1.6809 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)