Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.161 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.054 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.84 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoO2 + Tl2O3 + Co3O4 |
Band Gap0.523 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 307.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 165.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 213.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 355.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 309.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 213.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 243.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 213.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 165.8 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 232.3 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 71.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 213.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 284.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 118.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 232.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 71.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 71.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 165.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 165.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 189.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 331.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 142.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 23.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 284.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 165.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 284.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 355.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 331.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 232.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 71.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 142.1 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 309.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 243.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 213.1 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 232.3 |
SiC (mp-7631) | <1 0 1> | <1 0 1> | 243.0 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 154.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 165.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 23.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 309.8 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 94.7 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 165.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 355.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 213.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 189.4 |
C (mp-66) | <1 1 0> | <1 0 0> | 309.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 284.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 284.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 355.2 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 355.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CdGeO3 (mp-8275) | 0.1772 | 0.022 | 3 |
CdCoO3 (mp-770662) | 0.2226 | 0.065 | 3 |
MnAgO3 (mp-776486) | 0.3070 | 0.071 | 3 |
ZnSiO3 (mp-1020623) | 0.2200 | 0.148 | 3 |
NaSbO3 (mp-4482) | 0.3152 | 0.000 | 3 |
LiMnOF2 (mp-765319) | 0.4487 | 0.107 | 4 |
Li2ZrTeO6 (mp-6782) | 0.4750 | 0.012 | 4 |
Na2GeTeO6 (mp-10340) | 0.3621 | 0.000 | 4 |
Mn2Nb2Zn2O9 (mvc-12113) | 0.5268 | 0.019 | 4 |
Zn2MoWO6 (mvc-6039) | 0.5259 | 0.027 | 4 |
Pb2O3 (mp-20078) | 0.4828 | 0.009 | 2 |
SnO2 (mvc-6946) | 0.5235 | 0.162 | 2 |
Zn3N2 (mp-9460) | 0.5450 | 0.000 | 2 |
PtO2 (mp-1285) | 0.5445 | 0.000 | 2 |
CeSe2 (mp-1080328) | 0.5444 | 0.121 | 2 |
Li4ZrNb(TeO6)2 (mp-756177) | 0.4810 | 0.058 | 5 |
Li4Fe2TeWO12 (mp-768021) | 0.5803 | 0.083 | 5 |
LaZnFeCuO6 (mvc-9037) | 0.6081 | 0.292 | 5 |
Li4Cr2TeWO12 (mp-775566) | 0.5673 | 0.080 | 5 |
Li4Mn2TeWO12 (mp-768044) | 0.5749 | 0.056 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Tl_d Co O |
Final Energy/Atom-5.2281 eV |
Corrected Energy-60.2424 eV
-60.2424 eV = -52.2806 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)