Final Magnetic Moment1.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.067 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.203 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Fe3(PO4)4 + CO2 + LiFe(CO3)2 + Li3PO4 + O2 |
Band Gap0.013 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 332.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 199.5 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 217.2 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 207.7 |
ZnSe (mp-1190) | <1 1 1> | <1 0 1> | 297.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 278.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 297.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 266.0 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 266.0 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 199.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 1> | 198.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 332.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 332.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 266.0 |
BN (mp-984) | <1 1 1> | <1 0 -1> | 278.6 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 0> | 257.7 |
Al (mp-134) | <1 0 0> | <1 0 -1> | 278.6 |
Al (mp-134) | <1 1 0> | <1 0 1> | 297.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 332.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 66.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 217.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 199.5 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 266.0 |
TeO2 (mp-2125) | <0 0 1> | <1 -1 0> | 257.7 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 278.6 |
SiC (mp-7631) | <0 0 1> | <1 -1 0> | 257.7 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 0> | 217.2 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 108.6 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 207.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 332.5 |
TiO2 (mp-2657) | <1 0 0> | <1 1 1> | 264.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 332.5 |
C (mp-66) | <1 0 0> | <1 1 -1> | 244.1 |
C (mp-66) | <1 1 0> | <1 -1 0> | 257.7 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 207.7 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 198.1 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 276.9 |
GaAs (mp-2534) | <1 1 1> | <1 0 1> | 297.1 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 332.5 |
GaN (mp-804) | <0 0 1> | <1 -1 0> | 171.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 332.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 332.5 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 207.7 |
PbS (mp-21276) | <1 1 1> | <1 0 1> | 297.1 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 207.7 |
InP (mp-20351) | <1 1 1> | <1 0 1> | 297.1 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 332.5 |
SiC (mp-11714) | <0 0 1> | <1 -1 0> | 257.7 |
SiC (mp-11714) | <1 0 0> | <1 -1 0> | 257.7 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 199.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3V(BO2)5 (mp-770344) | 0.6315 | 0.111 | 4 |
Na3Ca(BO2)5 (mp-542719) | 0.6423 | 0.000 | 4 |
Na3Ca(BO2)5 (mp-614628) | 0.6454 | 0.002 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.6286 | 0.092 | 4 |
ZnAg3P3O13 (mvc-10277) | 0.6229 | 0.089 | 4 |
Li3Fe2P2(CO7)2 (mp-769710) | 0.1537 | 0.041 | 5 |
Li3Fe2P2(CO7)2 (mp-770266) | 0.1293 | 0.213 | 5 |
Li3Fe2P2(CO7)2 (mp-770153) | 0.1057 | 0.169 | 5 |
Li3Fe2P2(CO7)2 (mp-770052) | 0.1503 | 0.163 | 5 |
Li3Fe2P2(CO7)2 (mp-770292) | 0.1428 | 0.318 | 5 |
Li12VCr3P4(CO7)4 (mp-767735) | 0.6910 | 0.075 | 6 |
KLiMnPCO7 (mp-764256) | 0.6375 | 0.000 | 6 |
Li6MnNiP2(CO7)2 (mp-767293) | 0.6950 | 0.046 | 6 |
Li6VCrP2(CO7)2 (mp-767288) | 0.6941 | 0.080 | 6 |
NaLiMnPCO7 (mp-763833) | 0.6338 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv P C O |
Final Energy/Atom-6.6723 eV |
Corrected Energy-337.5219 eV
-337.5219 eV = -306.9258 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|