Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.738 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.101 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.36 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiBO2 + LiTi2O4 + Li6B4O9 + TiB2 |
Band Gap0.623 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 -1> | 125.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 209.2 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 -1> | 125.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 80.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 160.2 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 270.3 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 251.3 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 251.7 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 261.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 248.8 |
AlN (mp-661) | <0 0 1> | <1 0 -1> | 125.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 80.1 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 202.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 200.3 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 280.4 |
BaF2 (mp-1029) | <1 0 0> | <1 1 -1> | 274.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 280.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 313.9 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 280.4 |
GaN (mp-804) | <0 0 1> | <1 -1 1> | 197.6 |
GaN (mp-804) | <1 0 1> | <0 1 -1> | 253.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 284.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 280.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 240.3 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 240.3 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 200.3 |
SiO2 (mp-6930) | <1 1 1> | <1 -1 1> | 263.5 |
KCl (mp-23193) | <1 0 0> | <1 1 -1> | 274.6 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 200.3 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 240.3 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 248.8 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 254.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 200.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 284.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 313.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 160.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 169.2 |
InAs (mp-20305) | <1 0 0> | <1 1 -1> | 274.6 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 188.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 319.9 |
Te2W (mp-22693) | <0 1 1> | <0 1 -1> | 296.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 280.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 319.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 188.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 319.9 |
YVO4 (mp-19133) | <0 0 1> | <1 -1 1> | 197.6 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 280.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 313.9 |
YVO4 (mp-19133) | <1 1 1> | <0 1 0> | 80.1 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 200.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3BO3 (mp-27275) | 0.6469 | 0.000 | 3 |
Zn3(BO3)2 (mp-542833) | 0.6348 | 0.019 | 3 |
Na2CoO3 (mp-777186) | 0.6048 | 0.182 | 3 |
Zn3(BO3)2 (mp-559949) | 0.6270 | 0.019 | 3 |
Na3CoO3 (mp-777919) | 0.6632 | 0.018 | 3 |
Li3Mn(BO3)2 (mp-770903) | 0.4306 | 0.036 | 4 |
Li3V(BO3)2 (mp-779831) | 0.3912 | 0.052 | 4 |
Li3Sn(BO3)2 (mp-770286) | 0.4098 | 0.070 | 4 |
Li3Bi(BO3)2 (mp-777851) | 0.3814 | 0.086 | 4 |
LiZnBO3 (mp-758855) | 0.4304 | 0.015 | 4 |
Li4MnFe3(BO3)4 (mp-779072) | 0.6191 | 0.024 | 5 |
Li2MnFe(BO3)2 (mp-773762) | 0.5992 | 0.019 | 5 |
Li4MnFe3(BO3)4 (mp-773551) | 0.6087 | 0.024 | 5 |
Li2MnFe(BO3)2 (mp-850761) | 0.6228 | 0.018 | 5 |
Li2MnFe(BO3)2 (mp-781069) | 0.5853 | 0.018 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Ti_pv B O |
Final Energy/Atom-7.1095 eV |
Corrected Energy-179.0566 eV
-179.0566 eV = -170.6291 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)