Final Magnetic Moment1.385 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.449 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.212 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSO3 + NiSO4 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 221.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 295.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 221.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 147.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 73.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 206.4 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 221.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 103.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 221.8 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 295.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 221.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 295.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 295.7 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 103.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 109.6 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 206.4 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 73.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 -1> | 103.2 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 206.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 219.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 295.7 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 206.4 |
C (mp-66) | <1 1 1> | <1 0 0> | 221.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 73.9 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 103.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 221.8 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 73.9 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 295.7 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 147.8 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 103.2 |
PbS (mp-21276) | <1 1 0> | <1 0 -1> | 103.2 |
InP (mp-20351) | <1 1 0> | <1 0 -1> | 103.2 |
Au (mp-81) | <1 0 0> | <1 0 -1> | 103.2 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 221.8 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 147.8 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 221.8 |
CdWO4 (mp-19387) | <1 1 0> | <0 1 0> | 203.8 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 219.2 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 219.2 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 295.7 |
GaSb (mp-1156) | <1 1 0> | <1 0 0> | 221.8 |
GaTe (mp-542812) | <0 0 1> | <1 0 1> | 155.9 |
Al2O3 (mp-1143) | <1 1 0> | <0 0 1> | 109.6 |
Al2O3 (mp-1143) | <1 1 1> | <1 0 0> | 221.8 |
ZnTe (mp-2176) | <1 1 0> | <1 0 0> | 221.8 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 221.8 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 -1> | 206.4 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 295.7 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 295.7 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 147.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni2(SO4)3 (mp-779193) | 0.2128 | 0.160 | 3 |
CrP2O7 (mvc-14928) | 0.3804 | 0.198 | 3 |
NiP2O7 (mvc-15036) | 0.3682 | 0.227 | 3 |
V2(SO4)3 (mp-25724) | 0.2505 | 0.030 | 3 |
NiP2O7 (mp-540273) | 0.3850 | 0.227 | 3 |
SnPHO5 (mp-775543) | 0.4282 | 0.000 | 4 |
TePHO5 (mp-756804) | 0.4391 | 0.070 | 4 |
NbPHO5 (mp-756508) | 0.3759 | 0.088 | 4 |
LiMn2(SO4)3 (mp-770484) | 0.4425 | 0.514 | 4 |
TiPHO5 (mp-754297) | 0.4441 | 0.025 | 4 |
Cr19O48 (mp-850874) | 0.7101 | 0.167 | 2 |
V5O12 (mp-776915) | 0.7477 | 0.032 | 2 |
Cr19O48 (mp-780521) | 0.6975 | 0.085 | 2 |
Cr5O12 (mp-19575) | 0.4850 | 0.142 | 2 |
Cr3O8 (mp-557959) | 0.6701 | 0.048 | 2 |
Mn3VTe2(PO4)6 (mp-782657) | 0.4529 | 0.086 | 5 |
MnVP2(HO5)2 (mp-766980) | 0.4682 | 0.046 | 5 |
VFeP2(HO5)2 (mp-765969) | 0.4555 | 0.052 | 5 |
Zr2P3H4NO12 (mp-39770) | 0.4698 | 0.000 | 5 |
TiMn3Te2(PO4)6 (mp-765557) | 0.4422 | 0.086 | 5 |
LiMnVP2(HO5)2 (mp-765378) | 0.6228 | 0.046 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5889 | 0.003 | 6 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.5951 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.6280 | 0.001 | 6 |
LiMnVP2(HO5)2 (mp-765324) | 0.6005 | 0.046 | 6 |
Al2P2H8C2NO8F (mp-708964) | 0.6537 | 0.050 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Ni_pv S O |
Final Energy/Atom-5.4847 eV |
Corrected Energy-216.1500 eV
Uncorrected energy = -186.4800 eV
Composition-based energy adjustment (-0.503 eV/atom x 6.0 atoms) = -3.0180 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-2.541 eV/atom x 4.0 atoms) = -10.1640 eV
Corrected energy = -216.1500 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)