Final Magnetic Moment8.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.652 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.080 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.17 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBiO2 + MnO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 263.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 321.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 234.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 321.8 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 200.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 204.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 234.0 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 96.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 204.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 204.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 263.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 204.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 204.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 117.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 351.0 |
Al (mp-134) | <1 1 0> | <0 0 1> | 117.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 166.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 288.0 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 204.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 87.8 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 166.3 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 288.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 204.8 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 288.0 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 234.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 96.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 234.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 288.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 204.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 321.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 263.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 234.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 96.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 146.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 117.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 204.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 351.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 204.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 204.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 146.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 87.8 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 96.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 321.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 96.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 288.0 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 200.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 263.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 321.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn3SnO8 (mp-770865) | 0.3406 | 0.089 | 3 |
Co3BiO8 (mp-771742) | 0.1582 | 0.086 | 3 |
Mn3BiO8 (mp-773993) | 0.2263 | 0.060 | 3 |
Co3BiO8 (mp-774284) | 0.2332 | 0.071 | 3 |
Mn3SnO8 (mp-850479) | 0.3214 | 0.096 | 3 |
CaNiWO6 (mvc-14986) | 0.4740 | 0.303 | 4 |
Mn3Co3(SnO8)2 (mp-770554) | 0.5583 | 0.061 | 4 |
Mn3Nb2Co3O16 (mp-851279) | 0.5475 | 0.066 | 4 |
Ti2Mn3Co3O16 (mp-771910) | 0.5970 | 0.059 | 4 |
Mn3Cr3(SnO8)2 (mp-771095) | 0.5993 | 0.083 | 4 |
FeO2 (mvc-11993) | 0.5165 | 0.256 | 2 |
BiO2 (mvc-4364) | 0.4938 | 0.186 | 2 |
FeO2 (mvc-15000) | 0.5062 | 0.277 | 2 |
MoO2 (mp-715482) | 0.5121 | 0.256 | 2 |
VO2 (mvc-11624) | 0.5360 | 0.162 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv Bi O |
Final Energy/Atom-6.6772 eV |
Corrected Energy-90.7877 eV
-90.7877 eV = -80.1268 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 5.0426 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)