Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.393 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCrO2 + LiGaO2 |
Band Gap3.091 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 291.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 298.5 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 175.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 121.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 243.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 243.7 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 213.2 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 213.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 233.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 243.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 229.8 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 274.0 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 365.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 152.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 152.3 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 229.9 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 157.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 91.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 243.7 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 213.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 153.2 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 229.8 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 274.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 213.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 -1> | 229.9 |
DyScO3 (mp-31120) | <1 1 1> | <1 1 1> | 274.0 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 274.1 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 274.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 243.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 199.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 365.5 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 248.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 335.0 |
CdS (mp-672) | <1 0 1> | <1 1 -1> | 229.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 274.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 121.7 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 58.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 199.0 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 157.2 |
YVO4 (mp-19133) | <1 0 1> | <1 0 -1> | 291.5 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 314.4 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 149.2 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 274.0 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 335.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 248.7 |
Al (mp-134) | <1 1 1> | <1 0 0> | 365.5 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 174.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 121.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 60.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 121.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaTlO2 (mp-3056) | 0.0368 | 0.000 | 3 |
LiCrO2 (mp-772487) | 0.0450 | 0.002 | 3 |
NaCdO2 (mp-754567) | 0.0380 | 0.025 | 3 |
LiCrO2 (mp-18793) | 0.0364 | 0.000 | 3 |
LiNiO2 (mp-554862) | 0.0546 | 0.012 | 3 |
Li4Cr3GaO8 (mp-770277) | 0.0484 | 0.083 | 4 |
Li2CrFeO4 (mp-770193) | 0.0480 | 1.011 | 4 |
Li3Cr2FeO6 (mp-773312) | 0.0466 | 0.676 | 4 |
Li2CrFeO4 (mp-769983) | 0.0480 | 1.012 | 4 |
Li4CrFe3O8 (mp-769753) | 0.0489 | 1.511 | 4 |
Bi2Te3 (mp-568390) | 0.2084 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.2029 | 0.530 | 2 |
VO (mp-714885) | 0.2335 | 0.018 | 2 |
PbS (mp-1057015) | 0.2546 | 0.001 | 2 |
In2Se3 (mp-20830) | 0.2065 | 0.530 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6705 | 0.005 | 5 |
Hg (mp-982872) | 0.2819 | 0.020 | 1 |
Se (mp-7755) | 0.3419 | 0.181 | 1 |
Te (mp-10654) | 0.3227 | 0.047 | 1 |
Te (mp-105) | 0.2994 | 0.047 | 1 |
P (mp-53) | 0.3718 | 0.144 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Ga_d O |
Final Energy/Atom-6.6145 eV |
Corrected Energy-234.9781 eV
-234.9781 eV = -211.6635 eV (uncorrected energy) - 12.0780 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)