Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.409 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.092 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.34 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi6B4O9 + Sb2O3 |
Band Gap2.708 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 242.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 289.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 242.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 145.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 290.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 193.8 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 242.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 145.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 242.3 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 289.7 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 145.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 339.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 171.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 285.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 242.3 |
AlN (mp-661) | <1 1 1> | <1 1 -1> | 112.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 145.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 242.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 242.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 290.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 285.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 285.4 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 342.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 285.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 285.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 290.8 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 289.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 339.2 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 285.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 285.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 339.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 242.3 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 145.4 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 285.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 290.8 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 224.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 171.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 285.4 |
BN (mp-984) | <1 0 1> | <0 1 0> | 342.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 48.5 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 146.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 290.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 193.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 242.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 285.4 |
CdTe (mp-406) | <1 0 0> | <1 1 -1> | 224.4 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 285.4 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 224.6 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 242.3 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 48.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ag2CO3 (mp-676581) | 0.5955 | 0.030 | 3 |
Li3BO3 (mp-27275) | 0.5539 | 0.000 | 3 |
Li6B4O9 (mp-768875) | 0.5335 | 0.063 | 3 |
Na3CoO3 (mp-777919) | 0.5614 | 0.127 | 3 |
Li6B4O9 (mp-1020024) | 0.5340 | 0.000 | 3 |
Li3Bi(BO3)2 (mp-768771) | 0.1327 | 0.041 | 4 |
Li3V(BO3)2 (mp-772628) | 0.4497 | 0.059 | 4 |
LiZnBO3 (mp-758855) | 0.4511 | 0.015 | 4 |
Li3In(BO3)2 (mp-556799) | 0.3740 | 0.014 | 4 |
LiCuCO3 (mp-757800) | 0.4264 | 0.082 | 4 |
Li4Mn2Fe(BO3)4 (mp-767650) | 0.5273 | 0.319 | 5 |
Li4MnFe2(BO3)4 (mp-767642) | 0.5033 | 0.055 | 5 |
Li8Mn3Fe5(BO3)8 (mp-778883) | 0.5331 | 0.015 | 5 |
Li2MnFe(BO3)2 (mp-774078) | 0.5317 | 0.016 | 5 |
Li2MnFe(BO3)2 (mp-773762) | 0.5421 | 0.019 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv B Sb O |
Final Energy/Atom-6.4664 eV |
Corrected Energy-327.2402 eV
-327.2402 eV = -310.3852 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)