Final Magnetic Moment1.137 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.244 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.059 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Mn3(PO4)4 + MnO2 + CO2 + Li3PO4 |
Band Gap0.305 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 216.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 262.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 328.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 328.5 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 261.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 206.5 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 216.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 276.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 197.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 328.5 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 261.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 195.6 |
Te2Mo (mp-602) | <0 0 1> | <1 -1 0> | 253.1 |
GaSe (mp-1943) | <0 0 1> | <1 -1 0> | 253.1 |
Bi2Se3 (mp-541837) | <1 0 1> | <1 -1 0> | 253.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 328.5 |
Al (mp-134) | <1 0 0> | <0 1 -1> | 276.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 197.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 328.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 328.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 328.5 |
LiGaO2 (mp-5854) | <0 1 1> | <1 1 0> | 216.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 197.1 |
LiGaO2 (mp-5854) | <1 1 1> | <1 -1 0> | 168.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 262.8 |
Fe3O4 (mp-19306) | <1 0 0> | <1 1 0> | 216.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 328.5 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 197.1 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 273.4 |
C (mp-66) | <1 0 0> | <1 1 -1> | 245.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 328.5 |
BN (mp-984) | <1 0 0> | <1 -1 0> | 253.1 |
BN (mp-984) | <1 0 1> | <0 1 -1> | 184.2 |
BN (mp-984) | <1 1 1> | <0 1 -1> | 276.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 328.5 |
LaF3 (mp-905) | <1 1 1> | <0 0 1> | 197.1 |
MoS2 (mp-1434) | <1 0 1> | <0 1 -1> | 276.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 65.7 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 273.4 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 108.2 |
MgO (mp-1265) | <1 1 0> | <0 1 -1> | 276.2 |
TiO2 (mp-2657) | <1 0 0> | <1 1 1> | 261.1 |
C (mp-66) | <1 1 0> | <0 1 0> | 273.4 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 205.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 197.1 |
BaTiO3 (mp-5986) | <0 0 1> | <1 -1 0> | 253.1 |
BaTiO3 (mp-5986) | <1 1 0> | <1 -1 1> | 213.8 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 197.1 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 273.4 |
SiC (mp-11714) | <1 0 0> | <1 -1 0> | 253.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P C O |
Final Energy/Atom-7.0009 eV |
Corrected Energy-348.4296 eV
-348.4296 eV = -322.0420 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)