Final Magnetic Moment8.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.250 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.585 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.21 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCrO2 + Li4CrFe3O8 |
Band Gap2.308 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 -1> | 288.7 |
AlN (mp-661) | <0 0 1> | <0 1 -1> | 231.0 |
AlN (mp-661) | <1 1 0> | <1 1 -1> | 270.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 141.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 260.0 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 309.0 |
GaAs (mp-2534) | <1 0 0> | <0 1 -1> | 231.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 -1> | 270.6 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 240.0 |
BaF2 (mp-1029) | <1 1 1> | <1 1 -1> | 270.6 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 294.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 288.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 144.4 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 181.0 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 133.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 86.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 -1> | 270.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 241.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 301.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 231.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 260.0 |
KCl (mp-23193) | <1 1 1> | <1 1 -1> | 270.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 202.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 231.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 -1> | 288.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 283.9 |
InAs (mp-20305) | <1 1 0> | <1 1 -1> | 270.6 |
InAs (mp-20305) | <1 1 1> | <1 1 -1> | 270.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 288.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 120.0 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 60.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 154.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 -1> | 231.0 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 240.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 240.0 |
Te2W (mp-22693) | <0 1 0> | <1 -1 -1> | 278.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 317.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 202.2 |
CdS (mp-672) | <1 1 1> | <0 1 1> | 301.7 |
Te2Mo (mp-602) | <1 0 0> | <1 -1 -1> | 278.2 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 60.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 317.7 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 181.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 144.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 86.7 |
Te2Mo (mp-602) | <0 0 1> | <1 -1 -1> | 208.7 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 123.8 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 120.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 120.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 317.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NaYbO2 (mp-752924) | 0.1289 | 0.095 | 3 |
LiFeO2 (mp-19419) | 0.1349 | 0.075 | 3 |
Ba2PCl (mp-27869) | 0.1314 | 0.000 | 3 |
Li2PtO3 (mp-531826) | 0.1349 | 0.000 | 3 |
LiCoO2 (mp-24850) | 0.1407 | 0.193 | 3 |
Li4Cr3FeO8 (mp-770257) | 0.0721 | 0.788 | 4 |
Li4Cr3FeO8 (mp-770224) | 0.0747 | 0.519 | 4 |
Li4Cr3FeO8 (mp-770085) | 0.0724 | 0.521 | 4 |
Li2CrFeO4 (mp-770058) | 0.0638 | 1.418 | 4 |
Li2CrFeO4 (mp-770042) | 0.0751 | 1.459 | 4 |
LiTe3 (mp-27466) | 0.2897 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.1934 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.2032 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.1976 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.2453 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.5668 | 0.139 | 5 |
Hg (mp-982872) | 0.3594 | 0.020 | 1 |
Sb (mp-632286) | 0.4196 | 0.059 | 1 |
Se (mp-7755) | 0.4252 | 0.181 | 1 |
Te (mp-10654) | 0.3960 | 0.047 | 1 |
Te (mp-105) | 0.3353 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Fe_pv O |
Final Energy/Atom-6.6414 eV |
Corrected Energy-241.3056 eV
-241.3056 eV = -212.5249 eV (uncorrected energy) - 17.5440 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)