Final Magnetic Moment9.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.381 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.043 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.72 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3Mn3(PO4)4 + MnO2 + MnCO3 + CO2 + Li3PO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 307.9 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 123.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 327.7 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 196.6 |
AlN (mp-661) | <1 1 1> | <1 0 -1> | 329.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 307.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 307.9 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 196.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 246.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 262.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 246.3 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 196.6 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 65.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 61.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 307.9 |
BN (mp-984) | <1 0 1> | <1 0 0> | 262.2 |
Al (mp-134) | <1 0 0> | <0 0 1> | 246.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 196.6 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 196.6 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 131.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 61.6 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 184.8 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 257.9 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 307.9 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 262.2 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 257.9 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 196.6 |
C (mp-66) | <1 0 0> | <0 0 1> | 307.9 |
C (mp-66) | <1 1 0> | <1 0 0> | 327.7 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 327.7 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 1> | 211.5 |
Mg (mp-153) | <1 0 0> | <1 0 -1> | 65.8 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 307.9 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 196.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 307.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 327.7 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 123.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 327.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 327.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 123.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 257.9 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 257.9 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 307.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 257.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 65.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 307.9 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 184.8 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 211.5 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 217.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 307.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3Fe3(BO3)4 (mp-767662) | 0.6708 | 0.088 | 4 |
Li3Co(BO2)5 (mp-770196) | 0.7383 | 0.110 | 4 |
Na3Ca(BO2)5 (mp-542719) | 0.7203 | 0.000 | 4 |
Na3Ca(BO2)5 (mp-614628) | 0.7020 | 0.002 | 4 |
Li3Ni(BO2)5 (mp-771081) | 0.6844 | 0.061 | 4 |
Li5Mn2P2(CO7)2 (mp-771383) | 0.2353 | 0.041 | 5 |
Li5Mn2P2(CO7)2 (mp-771378) | 0.2120 | 0.047 | 5 |
Li5Mn2P2(CO7)2 (mp-770319) | 0.2266 | 0.047 | 5 |
Li5Mn2P2(CO7)2 (mp-770317) | 0.2505 | 0.048 | 5 |
Li5Mn2P2(CO7)2 (mp-770157) | 0.2211 | 0.045 | 5 |
Li12V3CrP4(CO7)4 (mp-767729) | 0.3378 | 0.070 | 6 |
Li12Mn3VP4(CO7)4 (mp-767666) | 0.3439 | 0.054 | 6 |
Li12MnCo3P4(CO7)4 (mp-767749) | 0.3238 | 0.044 | 6 |
Li6MnNiP2(CO7)2 (mp-767293) | 0.3378 | 0.046 | 6 |
Li6VCrP2(CO7)2 (mp-767288) | 0.3422 | 0.080 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv P C O |
Final Energy/Atom-6.9103 eV |
Corrected Energy-371.9035 eV
-371.9035 eV = -345.5159 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)